A method for preparing cathode material for use in lithium secondary batteries comprising the steps of: (a) mixing first and second reactants in a appropriate stoichiometric ratio to form a reaction mixture, wherein the first reactant is represented by Li x MO 2 , M is either Ni or Co, and x is a variable from 0.25 to 1.1, and the second reactant is V 2 O 3 ; V 2 O 5 , or NH 4 VO 3 , and (b) sintering the mixture in air at temperatures between 650° C.˜700° C. for 1˜2 hours to obtain a cathode material represented by LiMVO 4 . The first reactant can be obtained by an aqueous-phase reaction by mixing a first aqueous solution, which contains M(NO 3 ) 2 .6H 2 O, and a second aqueous, which contains LiOH.H 2 O, Li 2 O, Li 2 CO 3 , or Li(CH 3 COO), to form a precursory aqueous solution, and drying the precursory aqueous solution. Very high purity cathode materials can be obtained at a substantially reduced reaction time and substantially reduced reaction temperature, both of which will contribute to reduced production cost. The lithium secondary batteries so prepared can provide discharge voltages between 4.5˜4.9 volts.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 18.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for preparing cathode material for use in lithium secondary batteries comprising the steps of: (a) mixing first and second reactants, in a molar ratio of about 2 to 1, to form a reaction mixture, said first reactant being represented by Li x MO 2 , wherein M is either Ni or Co, and x is a variable form 0.25 to 1.1, and said second reactant being selected from the group consisting of V 2 O 3 , V 2 O 5 , and NH 4 VO 3 ; and (b) sintering said reaction mixture in air at temperatures between 650° C. and 700° C. for 1 to 2 hours to obtain an inverse spinel LiMVO 4 for use as a cath

  2. Claim 2Depends on #1

    The method for preparing cathode material for use in lithium secondary batteries according to claim 1 wherein said first reactant is Li x NiO 2 .

  3. Claim 3Independent Claim

    The method for preparing cathode material for use in l

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • H. M. Rietveld, "A Profile Refinement Method for Nuclear and Magnetic Structures" J. Appl. Cryst., no month, 1969, 65-71, No. 2.
  • H. M. Rietveld, A Profile Refinement Method for Nuclear and Magnetic Structures J. Appl. Cryst., no month, 1969, 65 71, No. 2.
  • J. C. Berneir et al., "Etude Cristallographique et magnetique de deux vanadates mixtes spinelles" Bull. Soc. Chim. France; 1963, no month, 1661-1666.
  • J. C. Berneir et al., tude Cristallographique et magn tique de deux vanadates mixtes spinelles Bull. Soc. Chim. France; 1963, no month, 1661 1666.
  • J. C. Bernier et al., "Academie des Sciences" Compt. Rendus., 253, 1961, no month, 1578.