Patents
US 5,456,771 A#33119623 Most CitedExpiredUnited States (USPTO)Utility

Thin Fe-Ni alloy sheet for shadow mask

3Forward Citations (#33119623 Global)
0.1/yrCitation Velocity (#45567057 Global)
1.06Citation PageRank (#38523746 Global)
24Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A thin Fe-Ni alloy sheet for shadow mask consists essentially of Ni of 34 to 38 wt. %, Si of 0.05 wt. % or less, B of 0.0005 wt. % or less, 0 of 0.002 wt. % or less and N of 0.0015% or less, the balance being Fe and inevitable impurities; said alloy sheet after annealing before press-forming having 0.2% proof stress of 28.5 kgf/mm2 or less; and a degree of {211} plane on a surface of said alloy sheet being 16% or less. And further modified similar alloy sheets are also provided. Further, a method for producing a thin Fe-Ni alloy sheet for shadow mask comprises the steps of: (a) hot-rolling of a slab into a hot-rolled alloy strip; (b) hot-rolled sheet annealing of the hot-rolled strip at 910 DEG to 990 DEG C.; (c) cold-rolling of the annealed hot-rolled strip into a cold-rolled strip; (d) recrystallization annealing of the cold-rolled strip; (e) finish cold-rolling of the recrystallization annealed strip at a finish cold reduction ratio in response to austenite grain size D(D mu m) yielded by the recrystallization annealing, the finish cold reducration ratio(R) being within a region enclosed by a range of R of 16 to 75 and a range of D of 6.38D-133.9</=R</=6.38D-51.0 and (f) a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 3.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A thin and annealed Fe-Ni alloy sheet suitable for forming a shadow mask by press forming the thin Fe-Ni alloy sheet, the thin Fe-Ni alloy sheet made of an alloy consisting essentially of Ni in an amount of 34 to 38 wt. % Si in an amount of 0.05 wt. % or less, B in an amount of 0.00001 to 0.0002 wt. %, O in an amount of 0.002 wt. % or less and N in an amount of 0.0015 wt. % or less, the balance being Fe and inevitable impurities; said alloy sheet after annealing and before press-forming having a 0.2% proof stress of 28.5 kgf/mm 2 or less; and the degree of the {211} plane on a surface of sa

  2. Claim 2Depends on #1

    The thin alloy sheet of claim 1, wherein said Si is from 0.001 to 0.05 wt. %, said O from 0.0001 to 0.002 wt. % and said N from 0.0001 to 0.0015 wt. %.

  3. Claim 3Independent Claim

    The thin alloy sheet of claim

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
EP 0,104,453 A1Shadow mask, color picture tube and color television—20
JP S5959861 AParts in electron tube—32
JP S6119737 AShadow mask base plate and its preparation—15
EP 0,174,196 A2Material for in-tube components & method of manufacture thereof—28
JP S61113747 AMaterial for shadow mask—15
DE 3,636,815 A1Shadow mask and process for producing shadow masks—28
DE 3,642,205 A1Shadow mask material and shadow mask—35
US 4,724,012 AMaterial for in-tube components and method of manufacturing it198820
US 4,751,424 AIron-nickel alloy shadow mask for a color cathode-ray tube198825
JP S63259054 AShadow mask—16
JP S6452024 AProduction of shadow mask material for cathode ray tube—9
WO 9,112,345 A1Thin sheet of iron-nickel alloy for shadow mask and production thereof—12
JP H03197645 ALead frame material—14
JP H03267320 AProduction of shadow mask material—13
FR 2,664,908 A1Feuille d'alliage fer-nickel pour masque de tube de television.—14
FR 2,668,498 A1Tole en alliage de fe-ni pour masque perfore, a aptitude au percage par gravure excellente, evitant le collage durant le recuit, et inhibant la production des gaz.—20
US 5,127,965 AFe-ni alloy sheet for shadow mask and method for manufacturing same199226
US 5,158,624 ASoft-magnetic nickel-iron-chromium alloy199218
US 5,207,844 AMethod for manufacturing an Fe-Ni cold-rolled sheet excellent in cleanliness and etching pierceability199316
EP 0,552,800 A1Thin metallic sheet for shadow mask—20
US 5,234,513 AFe-Ni alloy sheet excellent in hot workability, adhesivity to plating layer and solderability, and method for manufacturing same199323
US 5,234,512 AFe-ni alloy sheet for shadow mask, excellent in etching pierceability, preventing sticking during annealing, and inhibiting production of gases199324
EP 0,561,120 A1Thin Fe-Ni alloy sheet for shadow mask and method for manufacturing thereof—33
US 5,308,723 AThin metallic sheet for shadow mask199420

Non-Patent Literature (5)

  • Chemical Abstracts, p. 249, No. 133956d of JP A 60 251, vol. 104, No. 16, Apr. 21, 1986.
  • Chemical Abstracts, p. 249, No. 133956d of JP-A-60 251, vol. 104, No. 16, Apr. 21, 1986.
  • Database WPIL, Week 8610, Derwent Publications Ltd., London, GB; AN 86 066609 of JP A 61 019 737 (1986).
  • Database WPIL, Week 8610, Derwent Publications Ltd., London, GB; AN 86-066609 of JP-A-61 019 737 (1986).
  • Database WPIL, Week 8615, Derwent Publications Ltd., London, GB; AN 86 098295 & Abstract of JP A 61 044 126.