Method for manufacturing an Fe-Ni cold-rolled sheet excellent in cleanliness and etching pierceability

16Forward Citations (#5884566 Global)
0.5/yrCitation Velocity (#17402703 Global)
2.36Citation PageRank (#11125483 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for manufacturing an Fe-Ni alloy cold-rolled sheet excellent in cleanliness and etching pierceability, comprising: preparing an Fe-Ni molten alloy, containing 30 to 45 wt. % nickel, and subjected to dephosphorization and decarburization; adding aluminum and flux to the Fe-Ni molten alloy in a ladle made of an MgO-CaO refractory containing 20 to 45 wt. %; strongly stirring the Fe-Ni molten alloy which contains the added aluminum and flux in the ladle to produce a CaO-Al2O3-MgO slag so as to react the Fe-Ni molten alloy with the CaO-Al2O3-MgO slag to deoxidize the Fe-Ni molten alloy while controlling a value of activity of SiO2 from 0.001 to 0.005 and a value of activity of Al2O3 from 0.1 to 0.3 in the CaO-Al2O3-MgO slag, and the CaO-Al2O3-MgO slag having the following chemical composition: CaO and Al2O3: at least 57 wt. %, wherein the ratio of CaO/(CaO+Al2O3) being at least 0.45, MgO: up to 25 wt. %, SiO2: up to 15 wt. %, and oxides of metals having an oxygen affinity lower than that of silicon: up to 3 wt. % in total; casting the deoxidized Fe-Ni molten alloy into an ingot; and blooming, hot-rolling and cold-rolling the ingot to manufacture an Fe-Ni alloy cold-rolled sheet

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 16.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing an Fe-Ni alloy cold-rolled sheet excellent in cleanliness and etching pierceability, which comprises the steps of: preparing an Fe-Ni molten alloy, containing nickel in an amount within a range of from 30 to 45 wt. %, and subjected to dephosphorization and decarburization; adding aluminum and flux to said Fe-Ni molten alloy thus prepared, in a ladle made of an MgO-CaO refractory containing CaO in an amount within a range of from 20 to 40 wt. %; strongly stirring said Fe-Ni molten alloy which contains said added aluminum and flux in said ladle to produce a CaO-Al

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Patent Abstracts of Japan, vol. 10, No. 131 (C 346) (2188) May 15, 1986 of JP A 60 255 953 (Sumitomo Tokushiyu Kinzoku K. K.) Dec. 17, 1985.
  • Patent Abstracts of Japan, vol. 10, No. 131 (C-346) (2188) May 15, 1986 of JP-A-60-255 953 (Sumitomo Tokushiyu Kinzoku K. K.) Dec. 17, 1985.
  • Patent Abstracts of Japan, vol. 10, No. 182 (C 356) (2238) Jun. 25, 1986 of JP A 62 030 646 (Daido Steel Co. Ltd.) Feb. 12, 1986.
  • Patent Abstracts of Japan, vol. 10, No. 182 (C-356) (2238) Jun. 25, 1986 of JP-A-62-030 646 (Daido Steel Co. Ltd.) Feb. 12, 1986.
  • Patent Abstracts of Japan, vol. 10, No. 203 (C 360) (2259) Jul. 16, 1986 of JP A 61 044 156 (Nippon Mining Co. Ltd.) Mar. 3, 1986.