Copper-nickel-tin alloys for lead conductor materials for integrated circuits and a method for producing the same

43Forward Citations (#1209730 Global)
1.0/yrCitation Velocity (#7465606 Global)
13.02Citation PageRank (#684212 Global)
2Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Copper-nickel-tin alloys having high tensile strength and conductivity suitable for lead conductor materials for integrated circuits are produced by melting a starting material containing 0.5-3.0% by weight of Ni, 0.3-0.9% by weight of Sn, 0.01-0.2% by weight of phosphorus and 0-0.35% by weight of at least one of Mn and Si other than Cu, casting the molten metal, rolling conventionally the cast into a sheet having a thickness corresponding to more than 60% of cold reduction rate of the final necessary gauge, annealing such a rolled sheet at a temperature of 300-395 DEG C. for 1 hour, cold rolling the annealed sheet and annealing the cold rolled sheet at a temperature of 150-250 DEG C. for 1 hour.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 43.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Copper-nickel-tin alloys for electrical lead conductor materials for integrated circuits containing 0.5-3.0% by weight of Ni, 0.3-0.9% by weight of Sn, 0.01-0.05% by weight of P and 0-0.35% by weight of at least one of Mn and Si and the remainder copper.

  2. Claim 2Independent Claim

    A method for producing copper-nickel-tin alloys for electrical lead conductor materials for integrated circuits comprising as sequential steps melting a starting material containing 0.5-3.0% by weight of Ni, 0.3-0.9% by weight of Sn, 0.01-0.05% by weight of phosphorus and 0-0.35% by weight of at least one of Mn and Si and the remainder Cu; casting the molten metal; rolling the casting into a sheet having a thickness corresponding to more than 60% of cold reduction percent of the final necessary gauge; annealing said rolled sheet at a temperature of 300°-395° C. for 1 hour; cold