Patents
US 5,082,809 A#5003546 Most CitedExpiredUnited States (USPTO)Utility

High-strength alumina sintered body and process for preparation thereof

18Forward Citations (#5003546 Global)
0.5/yrCitation Velocity (#14887552 Global)
2.48Citation PageRank (#10276392 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a high-strength alumina sintered body which consists of 1 to 30% by weight, based on Al 2 O 3 and ZrO 2 , of ZrO 2 and 99 to 70% by weight, based on Al 2 O 3 and ZrO 2 , of Al 2 O 3 , and unavoidable impurities, said sintered body having a peak based on ZrO 2 at a position of a wave body having a peak based on ZrO 2 at a position of a wave number of 600±10 cm -1 in a measurement chart of the laser Raman spectrum analysis. This sintered body has a high flexural strength and a high breaking toughness in combination.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 18.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A high-strength alumina sintered body consisting of: 1 to 30% by weight, based on Al 2 O 3 and ZrO 2 , of ZrO 2 ; 99 to 70% by weight, based on Al 2 O 3 and ZrO 2 , of Al 2 O 3 ; and unavoidable impurities; said sintered body having a peak based on ZrO 2 at a position of a wave number of 600±10 cm -1 in a measurement chart of the laser Raman spectrum analysis.

  2. Claim 2Depends on #1

    A sintered body as set forth in claim 1, wherein the peak heigh ratio defined by the formula of (Hc/Ha)×100, in which Hc stands for the height of the peak based on ZrO 2 at a position of a wave number of 600+10 cm -1 and Ha stands for the height of the peak based on Al 2 O 3 at a wave number of 415 cm -1 or in the vicinity thereof, is at least 10.0.

  3. Claim 3Depends on #2

    A sintered body as set forth in claim 2, wherein the peak height ratio is at least 20.0.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 2012252655 A1Ceramic composite material consisting of aluminium oxide and zirconium oxide as main constitutents—6
US 9,630,883 B2Ceramic composite material consisting of aluminium oxide and zirconium oxide as the main constituents, and a dispersoid phase20172
US 5,625,256 AHigh-pressure discharge lamp having a ceramic discharge vessel, sintered body suitable therefor, and method for producing the sintered body199757
US 10,000,418 B2Refractory product, use of zirconium dioxide, zirconium dioxide, method for manufacturing a refractory product and a refractory product manufactured therewith20180
US 9,162,008 B2Ceramic manufactures20159
JP 2016132577 AAlumina-zirconia sintered body—3
US 6,194,336 B1Highly toughened alumina sintered bodies and their manufacturing process20018
US 8,074,472 B2Grinding beads and method of producing the same20110
CN 106,470,958 ARefractory product, the purposes of zirconium dioxide, zirconium dioxide, be used for the method manufacturing refractory product and the refractory product being produced from—3
US 2012292832 A1Ceramic manufactures—1
US 2012252656 A1Ceramic composite material consisting of aluminium oxide and zirconium oxide as the main constituents, and a dispersoid phase—17
US 2015313714 A1Ceramic Manufactures—0
US 2009036291 A1Grinding beads and method of producing the same—13
US 9,795,709 B2Ceramic composite material consisting of aluminium oxide and zirconium oxide as main constitutents20170
US 9,694,102 B2Ceramic manufactures20170