Patents
US 4,849,142 A#2364628 Most CitedExpiredUnited States (USPTO)Utility

Superplastic forging of zirconia ceramics

29Forward Citations (#2364628 Global)
0.8/yrCitation Velocity (#9525021 Global)
6.10Citation PageRank (#2397815 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to producing relatively flaw free zirconia ceramic shapes requiring little or no matching by superplastic forging of a fully sintered or partially sintered preform. The preform is prepared by providing a starting powder comprising by weight from about 70% to about 100% zirconia and from about 0 to about 30% of stabilizing additives, e.g. commerically available TZ-3Y powder, cold pressing to obtain a preform of green density ranging from about 30% of theoretical density to about 75% of theoretical density and partially or fully sintering at atmospheric pressure, e.g. in argon or air at a temperature ranging from about 900 DEG C. to about 1900 DEG C. The superplastic forging is carried out by isothermally pressing the partially or fully sintered preform into substantially final shape utilizing a temperature and strain rate such that surface cracks do not occur, e.g. utilizing a temperature of 1310 DEG C., a substantially constant displacement rate based on an initial strain rate of 7x10-3 seconds -1 and open die or closed die processing in a graphite or metal die.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 29.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing polycrystalline zirconia ceramic parts which are relatively flaw free and which need little or no machining, said process comprising the steps of: (a) providing a starting powder comprising by weight from about 70% to 100% zirconia and from 0 to about 30% of additives, (b) cold pressing to obtain a preform of a green density ranging from about 30% of theoretical density to about 75% of theoretical density, (c) sintering in an inert atmosphere or in air or in vacuum at a temperature ranging from about 900° C. to about 1900° C. to obtain a density which ranges from ab

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Alper, A. M., High Temperature Oxides, Part II, Academic Press (1970), pp. 117 166.
  • Alper, A. M., High Temperature Oxides, Part II, Academic Press (1970), pp. 117-166.
  • Alper, A. M., High temperature Oxides, Part III, Academic Press (1970), pp. 235 281.
  • Alper, A. M., High temperature Oxides, Part III, Academic Press (1970), pp. 235-281.
  • Baudelet, B. Superplasticity, Conference Internationale, Grenoble, France, 9/16 19/1985, pp. 16.1 16.19.