Patents
US 4,870,136 A#1626034 Most CitedExpiredUnited States (USPTO)Utility

Molecular oriented, silane-crosslinked ultra-high-molecular-weight polyethylene molded article and process for preparation thereof

37Forward Citations (#1626034 Global)
1.0/yrCitation Velocity (#6261173 Global)
3.57Citation PageRank (#5724110 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

If ultra-high-molecular-weight polyethylene having an intrinsic viscosity ( eta ) of at least 5 dl/g is grafted with a silane compound in the presence of a radical initiator and extrusion-molded and the extrudate is impregnated with a silanol condensation catalyst after or during drawing and is then exposed to water to effect crosslinking, there is obtained a novel molecularly oriented molded articles in which increase of the melting temperature, which is not observed in conventional draw-molded or crosslinked molded articles of polyethylene, can be attained, and even if this molecularly oriented molded article is exposed to a temperature of 180 DEG C. for 10 minutes, the molded article is not fused but the shape is retained and even after this heat history, a high strength retention ratio can be maintained. In this draw-molded article, the adhesiveness and creep resistance are prominently improved while high elastic modulus and high tensile strength inherent to a draw-molded article of ultra-high-molecular-weight polyethylene are retained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 37.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A molecularly oriented, silane-crosslinked ultra-high-molecular-weight polyethylene molded article, wherein when the molded article is analyzed in the constrained state by a differential scanning calorimeter, at least two crystal-melting peaks (Tp) appear at temperatures higher by at least 10° C. than the inherent crystal-melting temperature (Tm) of the ultra-high-molecular-weight polyethylene obtained as the main melting peak at the second temperature elevation and the melting calorific value of the crystal-melting peaks (Tp) is at least 50% of the total melting calorific value, and the sum o

  2. Claim 2Depends on #1

    A molded article as set forth in claim 1, wherein the heat

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗