Process for preparation of synthetic mordenite molded body
Abstract
A synthetic mordenite molded body is prepared by a process wherein a starting mixture comprising, as the main components, a silica source, an alumina source, an alkali source and water is molded into a starting molded body, the molded body is calcined and the calcined molded body is heated in an aqueous solution of sodium silicate. The starting mixture has incorporated therein a mordenite seed crystal powder. When the molded body is calcined, the temperature is elevated by heating to a calcination temperature not lower than 400 DEG C. at an average rate of at least 10 DEG C./min and calcination is conducted at the calcination temperature within a time period of 2 hours. When the calcined molded body is crystallized, an aqueous solution of sodium silicate having an SiO2 concentration of 7 to 25% by weight, an Na2O concentration of 2 to 8% by weight and an SiO2/Na2O molar ratio of from 0.9 to 4.0 is used as the aqueous solution of sodium silicate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 26.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An improvement in a process for the preparation of a synthetic mordenite molded body, which comprises molding a starting mixture consisting essentially of as the main components a silica source, an alumina source, an alkali source and water to obtain a starting molded body, calcining the molded body to obtain a calcined molded body and crystallizing the calcined molded body in an aqueous solution of sodium silicate, wherein the improvement comprises (a) making a mordenite seed crystal powder present in the starting mixture, in an amount of 0.1 to 10% by weight based on the starting mixture on
Technical Overview & Description