Method for the production of mordenite
Abstract
CRYSTALLINE ZEOLITES INCLUDING MORDENITE AND ANALCITE ARE PRODUCED BY HEATING AN ALKALI METAL SILICATE GLASS COMPRISING SIO2, M2O, AND AL2O3 WHEREIN M IS SODIUM OR POTASSIUM, THE MOLAR RATIO OF SIO2/M2O RANGING FROM ABOUT 1 TO 4 AND THE AL2O3 BEING PRESENT IN AN AMOUNT UP TO 10% BY WEIGHT (PREFERABLY 0.1-5%) BASED ON THE WEIGHT OF SIO2 AND M2O, IN WATER AT A TEMPERATURE OF FROM ABOUT 110 TO 210* C. UNTIL THE ZEOLITE PRODUCT FORMS. AUXILIARY RAW MATERIALS SUCH AS POWDERED SILICA SAND, SILICA SOL, SILICA GEL, DIATOMACEOUS EARTH, SODIUM OR POTASSIUM HYDROXIDES OR CARBONATES, SODIUM ALUMINATE, ALUMINUM HYDROXIDE, AND ALUMINA SOL CAN BE USED WITH THE ALKALI METAL SILICATE GLASS.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 7.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (0)