Annealing Group III-V compound doped silicon-germanium alloy for improved thermo-electric conversion efficiency
Abstract
The thermoelectric conversion efficiency of a GaP dope SiGe alloy is improved about 30 percent by annealing the alloy at a temperature above the melting point of the alloy, preferably stepwise from 1200 DEG C. to 1275 DEG C. in air to form large grains having a size over 50 mu m and to form a Ge-Ga-P rich phase and a silicon rich phase containing SiP and SiO2 particles.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 21.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing an improved thermoelectric element comprising the steps of: annealing an alloy of a Group IV material and a Group III-V compound at a temperature close to or above the solidus point.
- Claim 2Depends on #1
A method according to claim 1 in which the alloy contains from 0.1 to 10 mole percent mixture of Group III-V elements or compounds.
- Claim 3Depends on #2
A method according to claim 2 in which the Group III metal is selected from at least one of gallium, indium or aluminum and the Group V element is selected from at least one of phosphorous, antimony or arsenic.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (5)
- B. Abeles, D. S. Beers, G. D. Cody, and J. P. Dismukes, Phys. Rev., 125, 44, (1962).
- C. Wood, D. Zoltan and G. Stapfer, Rev. Sci. Instrum., 56, 5, (1985).
- D. M. Rowe and V. S. Shukula, J. Appl. Phys., 52 (12), 7421, (1981).
- H. R. Meddins and J. E. Parrott, J. Phys. C: Solid St. Phys., 9, 1263, (1976).
- J. P. Dismukes, L. Ekstrom, E. F. Steigmeier, I. Kudman and D. S. Beers, J. Appl. Phys., 35, 2899, (1964).