US 4,159,214 A#4076255 Most CitedExpiredUnited States (USPTO)Utility

Formation of heterojunctions utilizing back-side surface roughening for stress relief

20Forward Citations (#4076255 Global)
0.4/yrCitation Velocity (#18571488 Global)
8.38Citation PageRank (#1422238 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A crack free layer of GaP is epitaxially deposited on a silicon phosphide surface of a silicon substrate having an (III) orientation. The silicon substrate is prebaked on a carbide coated susceptor with palladium diffused hydrogen at about 1200° C. and pretreated with phosphine at about 1140° C. to form the silicon phosphide surface. The temperature is lowered to 800°-900° C. in the presence of phosphine and trimethyl gallium is introduced at a ratio of 1 to 10 with the phosphine. Cracks in the gallium phosphide are prevented by roughing the bottom non-phosphine. Cracks in the silicon substrate such that the roughed surface is under compressive stress and induces tensile stress on the phosphided surface to reduce the compressive stress reduced by gallium phosphide layer when the substrate is annealed at about 1200° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of relieving stress between two layers of different semiconductors, said semiconductors having different coefficients of thermal expansion, comprising roughening the surface of the layer with the lower coefficient of thermal expansion opposite the common surface of said two layers, annealing and cooling said lower coefficient of thermal expansion layer to produce compressive stress on the roughened surface and tensile stress on the common surface, and epitaxially depositing the semiconductor layer with the higher coefficient-of-thermal expansion.

  2. Claim 2Depends on #1

    The method according to claim 1 wherein said annealing is performed before the other layer is deposited at said common surface.

  3. Claim 3Depends on #1

    The method according to claim 1 wherein said lower coefficient thermal expansion layer is silicon and said other layer is III-V

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Bean et al., "Some Properties of Vapor Deposited SiC".
  • Blachman, A.G., "Use of Bias-Sputtered Film to Stress-Film" Ibid., vol. 15, No. 9, Feb. 1973, pp. 2701-2702.
  • Bratter et al., "Dielectric Structure as an Out-diffusion Barrier".
  • J. Electrochem. Soc., vol. 114, No. 11, Nov., 1967, pp. 1158-1161.
  • Wenzel, C., "Slip and Bowing Control - Techniques" SCP and Solid State Tech., Aug. 1967, pp. 40-44.