Magnetic head made from amorphous magnetic film

9Forward Citations (#10981933 Global)
0.2/yrCitation Velocity (#30236110 Global)
4.41Citation PageRank (#4063042 Global)
16Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A magnetic head comprising a magnetic film in at least a part of a magnetic circuit, at least a part of the magnetic film being formed in contact with, or being exposed to, an oxide or oxygen at least in a heating step at 150 DEG C. or higher in a process for preparing the magnetic head is disclosed. An amorphous alloy film for the magnetic film has the following composition formula to give distinguished head characteristics without any oxidation: CoaTbZrcNd where T is at last one of Nb, Ta, W, Mo, V and Cr; N is at least one of Au, Pt and Ag; d>/=1, b>0, b1+b2+2c>/=10, a+d>/=80, -1</=(3c-b1-3b2-5b3-3b4-4d)/(c+b1+b2+b3+b4+d)</=1, and a+b+c+d=100, where b1 is a Nb concentration, b2 is a Ta concentration, b3 is a W concentration, b4 is sum total of Mo, Cr and V concentrations and b=b1+b2+b3+b4.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 9.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A magnetic head comprising a magnetic circuit, at least a part of said magnetic circuit including a magnetic film, wherein said magnetic film is composed of an amorphous alloy film having the following composition formula: Co a T b Zr c N d wherein T is at least one of Nb, Ta, W, Mo, V, and Cr; N is at least one of Au, Pt and Ag; d≧1, b>0, b 1 +b 2 +2c≧10, a+d≧80, -1≦(3c-b 1 -3b 2 -5b 3 -3b 4 -4d)/(c+b 1 +b 2 +b 3 +b 4 +d)≦1, and a+b+c+d=100, where b 1 is a Nb concentration, b 2 is a Ta concentration, b 3 is a W concentration, b 4 is sum total of Mo, Cr and V concentrat

  2. Claim 2Depends on #1

    A magnetic head according to claim 1, wherein said magnetic film is formed in contact with an oxide layer and is subjected to a heating step at an elevated temperature of at least 150° C.