Abstract
A wound iron core formed by winding a thin strip of a soft magnetic alloy into a triodal form, characterized in that a Co-base amorphous magnetic alloy is used as the thin strip and that the thin strip is annealed in a magnetic field in the direction of excitation, so that the core exhibits a rectangle ratio Br/B 10 of 85% or higher in D.C. hysteresis curve. The Co-base amorphous magnetic alloy has a composition substantially expressed by: Co 100-a-b X a Y b where X represents one, two or more elements selected from a group consisting of Ti, V, Cr, Mn, Fe, Ni, Zr, Nb, Mo, Ru, Hf, Ta, W, Y, Ce, Pr, Nd, Sm, Eu, Gd, Tb and Dy, while Y represents one, two or more elements selected from a group consisting of B, C, Al, Si, P and Ge, and wherein the following conditions are met: 0≦ a ≦15 (atom%) and 14≦ b ≦30 (atom%).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 15.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.