Polymer composition having positive temperature coefficient characteristics
Abstract
A polymer composition having positive temperature coefficient characteristics is described, comprising 100 parts by weight of a mixture consisting of from 40 to 90% by weight of a crystalline polymer and from 60 to 10% by weight of an electrically conductive powder and from 10 to 300 parts by weight of a semiconductive inorganic substance. This polymer composition can withstand high voltage and when used as a heat generator, produces a uniform distribution of heat and has a long service life. Thus the polymer composition is useful for production of an overcurrent protecting element and a heat generator.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 30.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A polymer composition having positive temperature coefficient characteristics, comprising 100 parts by weight of a mixture consisting of from 40 by 90% by weight of a crystalline polymer and from 60 to 10% by weight of an electrically conductive powder having a particle diameter of from 10 to 200 μm and from 10 to 300 parts by weight of a semiconductive inorganic substance having a specific resistance of from 10 -2 to 10 8 ohm-cm and a particle diameter of not more than 300 μm.
- Claim 2Depends on #1
The polymer composition of claim 1, wherein the semiconductive inorganic substance is silicon carbide, boron carbide or a mixture thereof.
- Claim 3Independent Claim
A polymer composition having positive temperature coefficient characteristics, comprising 100 parts by weight of a mixture consisting of from 40 to 90% by weight of a crystalline polymer and fr
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗