Process for preparing semiconducting silicon carbide sintered body
Abstract
A silicon carbide sintered body exhibiting N-type semiconductivity is produced by shaping a mixture of β-silicon carbide, boron additive and a carbonaceous additive into a green body and sintering the body in an atmosphere containing nitrogen to produce a sintered body having a density of at least about 90% and pores which are substantially non-interconnecting.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 38.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing an N-type semiconductor having an electrical resistivity at 20° C. ranging from 10 ohm centimeters to 10 -2 ohm centimeter and an electrical resistance that shows a positive temperature coefficient at temperatures ranging from about 800° C. to about 2000° C. and which retains N-type semiconducting properties at temperatures ranging from about -100° C. to 2000° C. which comprises providing a substantially homogeneous mixture of a submicron powder consisting essentially of β-silicon carbide, an amount of boron additive selected from the group consisting of boron and boron
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗