Steel blackplate for surface treatment, having a soft temper degree of T-3 or less, and improved fluting resistance is produced by the combination of a chemical composition of 0.01% to 0.08% carbon, 0.015% or less phosphorus, without titanium and niobium; steelmaking without vacuum-degassing; a low slab-heating temperature of 1240 DEG C. or less; a coiling temperature of 620 DEG C. to 710 DEG C.; continuous annealing having a heat pattern to decrease the solute carbon and nitrogen; and skin-pass rolling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a soft blackplate for surface treatment, comprising the steps of: obtaining an aluminum-killed steel containing, by weight percentage, from 0.01% to 0.08% of carbon, from 0.05% to 0.60% of manganese, 0.02% or less of phosphorus, from 0.005% to 0.10% of acid-soluble aluminum, and 0.01% or less of nitrogen, the balance being essentially iron; forming a slab of the aluminum-killed steel by continuous casting or ingot-making followed by rough-rolling; heating the slab to a temperature of 950° C.-1240° C.; hot-rolling the heated slab to form a strip; coiling the stri

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • The Making, Shaping and Treating of Steel, United States Steel, 1971, p. 1000.