Process for producing deep-drawing cold rolled steel strips by short-time continuous annealing

13Forward Citations (#7577140 Global)
0.3/yrCitation Velocity (#25449410 Global)
2.52Citation PageRank (#10044054 Global)
13Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing a cold rolled steel strip having excellent workability by a short-time continuous annealing, which process is constituted by hot rolling a low carbon steel slab of steel having a carbon content of from about 0.003 to 0.08% into a steel strip; cold rolling the hot rolled steel strip; rapidly heating the cold rolled steel strip to a recrystallization temperature range at a heating rate not less than 40 DEG C./second; slowly heating the thus rapidly heated steel strip to an annealing temperature at a heating rate ranging from 5 DEG to 30 DEG C./second; annealing the thus slowly heated steel strip at an annealing temperature T which is no lower than 700 DEG C. and no higher than the A3 transformation temperature and for an annealing time t no shorter than [8-0.03 (T-680)] seconds and no longer than [80-0.15 (T-680)] seconds, initially slowly cooling the thus annealed steel strip at a cooling rate less than 50 DEG C./second, and then rapidly cooling the strip at a cooling rate not less than 50 DEG C./second from a temperature TQ ranging from higher than 600 DEG C. to no higher than [T-0.027 (T-680)( 2ROOT t+23.7)] DEG C. to an over-ageing temperature range; and s

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a cold rolled steel strip having excellent deep drawing properties by a short-time continuous annealing, which comprises: hot rolling a low carbon steel slab of steel having a carbon content of from about 0.003 to 0.08% into a steel strip; cold rolling the hot rolled steel strip; rapidly heating the cold rolled steel strip to a recrystallization temperature range at a heating rate not less than 40° C./second; slowly heating the thus rapidly heated steel strip to an annealing temperature at a heating rate ranging from 5° to 30° C./second; annealing the thus slowl