US 4,619,871 A#2770327 Most CitedExpiredUnited States (USPTO)Utility

Copper foil for printed circuit board

26Forward Citations (#2770327 Global)
0.7/yrCitation Velocity (#12150023 Global)
9.86Citation PageRank (#1086020 Global)
10Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A copper foil resistant to acids and heat and yet easy to etch is obtained by forming a cobalt layer containing molybdenum and/or tungsten on the bonding surface thereof. Roughening of the foil surface prior to formation of the layer provides highly peel-resistant bonding of the foil thereat to resin-containing substrates of the type found in typical printed circuit boards. The provision of a chromate layer on the cobalt further improves the adhesion between the copper foil and resin-containing substrates.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 26.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A copper foil, bonded to a resin-containing substrate to be a constituent of a printed circuit board, comprising: on that surface which is bonded to said substrate a coating cobalt layer containing at least one element selected from the group consisting of molybdenum and tungsten for improved bonding, higher resistance to chemicals and heat, and facility for etching, wherein said element is present in an amount in the range 5 to 40 percent by weight of all the metals contained in said layer.

  2. Claim 2Depends on #1

    A copper foil as claimed in claim 1, wherein: said coated surface of said copper foil is pre-roughened.

  3. Claim 3Depends on #1

    A copper foil as claimed in claim 1, wherein: the thickness of said layer is in the range 0.01 μm to 1.0 μm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Copper Foils and Electric Laminates", Chem. Abstracts 101:172572h, Jun. 1984.
  • "Corrosion Testing of a Cobalt-Molybdenum Alloy", Karavaev et al., Chem. Abstracts 93:56707y and 93:56708z, 1977.
  • "Electrodeposition of Tungsten and Molybdenum with Iron-Group Metals", Zak et al., Chem. Abstracts 92:171466k, 1979.
  • Copper Foils and Electric Laminates , Chem. Abstracts 101:172572h, Jun. 1984.
  • Corrosion Testing of a Cobalt Molybdenum Alloy , Karavaev et al., Chem. Abstracts 93:56707y and 93:56708z, 1977.