Peel strength enhancement of copper laminates 102426-201
Abstract
In one aspect, a copper foil (14, 60) for lamination to a dielectric substrate (62) includes a layer (64) deposited on a surface of the copper foil (14, 60). The layer (64) is formed from chromium and zinc ions or oxides and is treated with an aqueous solution containing at least 0.5% silane. In another aspect, a peel strength enhancement coating (64) is disposed between a copper foil (14, 60) laminate and a dielectric substrate (62). The peel strength enhancement coating (64) comprises a metal and metal oxide mixture containing a metal selected from groups 5B, 6B, and 7B of the periodic table of the elements. The effective thickness of the peel strength enhancement coating (64) is that thickness capable of providing less than or equal to 10% loss of peel strength, when measured in accordance with IPC-TM-650 Method 2.4.8.5 using a 1/8 inch wide test specimen, after being immersed in 4N HCl at about 60°C for 6 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,619,871 A | Copper foil for printed circuit board | 1986 | 26 |
| US 6,426,146 B1 | Treated copper foil and process for making treated copper foil | 2002 | 19 |
Non-Patent Literature (1)
- See also references of WO 2004053193A1