The strength of the stainless steel containing cementitious composite material of U.S. Pat. No. 4,482,385 is improved by curing it according to a specific schedule which includes the steps of curing in a mold, steam curing after demolding, slow drying and dry thermal curing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of increasing the strength of a cementitious composite material containing irregularly shaped stainless steel particles comprising: a. casting the composite material into a mold; b. permitting the cast material to remain in the mold for between 20 and 48 hours at ambient room conditions; c. demolding the cast material and steam curing the demolded material at 60° C. for at least 18 hours; d. slow drying the steam cured material for at least one day at ambient room conditions and then e. dry thermally curing the resulting material at an elevated temperature between 175° and 230

  2. Claim 2Depends on #1

    The method of claim 1 in which the temperature is about 205° C. and the dry thermal cure is for about 1.5 days.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗