Manufacture of cement-resin composite articles
Abstract
Cement-resin composite articles are manufactured by preparing cement articles from Portland cement having a high silicic modulus, or a mixture of 50 to 90% by weight of Portland cement and 50 to 10% by weight of siliceous reactive material, presetting the cement articles at ambient temperature, steam curing the articles under pressure at a temperature from 150° to 250° C. for 1 to 6 hours, subjecting the steam cured articles to a thermal treatment in an anhydrous environment at a temperature of 120°-350°C. for 1 to 12 hours, impregnating the resulting articles with a monomeric polymerizable substance, and polymerizing the monomeric substance. The monomeric substance may be styrene, methylmethacrylate, vinyl ester, or a mixture of copolymerizable monomers. The articles may be placed under vacuum before impregnation and impregnation may be conducted under elevated pressure.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 22.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for manufacturing cement articles having very high mechanical strength, comprising: a. forming articles of a desired shape from a member selected from the group consisting of mortar and concrete prepared from water and a member selected from the group consisting of Portland cement having a high silicic modulus, pozzolana cement and a mixture consisting of 50 to 90% by weight of Portland cement and 50 to 10% by weight of reactive siliceous material; b. pre-aging said articles at room temperature; c. steam-curing said articles in an autoclave at a temperature from 150° to 250° C. f
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗