Titanium nitride dispersion strengthened alloys
Abstract
To increase the creep strength of a titanium-containing alloy which also contains chromium, the alloy powder is heated in the presence of ammonia at a temperature of the order of 700° C. so as to form a layer of chromium nitride(s) on the particles and is then heated further in an inert atmosphere at a temperature between 1000° C. and 1150° C. to dissociate the chromium nitride(s) thereby effecting nitriding of the titanium to titanium nitride which affords dispersion-strengthening of the alloy.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Method for the production of titanium nitride dispersion strengthened alloys, such method including the steps of subjecting particles of titanium-containing alloy powder which also contains chromium to heating in the presence of ammonia to form a layer of chromium nitride(s) on the particles, and then to heating at a higher temperature and in an inert atmosphere to dissociate the chromium nitride(s) and to convert substantially all the titanium present to titanium nitride.
- Claim 2Depends on #1
Method according to claim 1, wherein the titanium-containing alloy powder is a titanium-containing stainless steel powder.
- Claim 3Depends on #1
A method according to claim 1, wherein the titanium-containing alloy powder is a titanium-containing nickel based alloy powder.
Technical Overview & Description