US 4,427,461 A#14245362 Most CitedExpiredUnited States (USPTO)Utility

Nitridation and brazing of assemblies with titanium-containing iron based alloys

7Forward Citations (#14245362 Global)
0.2/yrCitation Velocity (#35933277 Global)
3.04Citation PageRank (#7436517 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of internally nitriding and brazing assemblies having iron based components to which titanium has been internally added prior to casting. A brazed assembly includes iron based components to which titanium is added prior to casting and is dispersion strengthened by nitridation to form an array of titanium nitride particles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a brazed composite of a thin gauge nitride-strengthened titanium-containing iron-base alloy member with a second iron-base alloy member brazed thereto, comprising the sequential steps: (a) applying to a pre-formed thin gauge titanium containing iron-base alloy member which is pre-assembled to a second iron-based alloy member, a powdered brazing alloy melting in the temperature range of 1700° to 2200° F. and wettable on the surface of said members following nitridation. (b) heating said assemblage to a temperature in the range of about 1100° to 1400° F. in the presence

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗