Patents
US 4,581,079 A#4092173 Most CitedExpiredUnited States (USPTO)Utility

Bearing steel

20Forward Citations (#4092173 Global)
0.5/yrCitation Velocity (#15140328 Global)
6.47Citation PageRank (#2178346 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A bearing steel containing about 0.8% to about 1.2% carbon, about 0.5% to about 1.33% manganese, about 0.25% to about 0.7% silicon, about 0.14% to about 0.5% molybdenum, up to about 0.75% chromium and the balance essentially iron has improved hardenability and resistance to rolling contact fatigue than does the standard 52100 bearing steel.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A wrought steel in the spheroidized and hardened condition having high hardness and resistance to rolling contact fatigue consisting essentially, by weight, of about 0.8% to about 1.2% carbon, about 0.5% to about 1.33% manganese, about 0.25% to about 0.7% silicon, about 0.25% to about 0.5% molybdenum, up to about 0.75% chromium, up to about 0.01% aluminum, up to about 0.03% nitrogen, with the balance essentially iron, said steel demonstrating superior hardenability to that of standard SAE 52100 and showing substantially no evidence of graphitization after a long spheroidize-annealing cycle.

  2. Claim 2Depends on #1

    A steel in accordance with claim 1 containing at least about 0.25% chromium and not more than about 0.5% silicon.

  3. Claim 3Depends on #1

    A steel in accordance with claim 1 consisting essentially of about 0.95% to about 1.15% carbon, about 0.5

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗