Bearing steel composition

34Forward Citations (#1803820 Global)
0.6/yrCitation Velocity (#12457730 Global)
15.19Citation PageRank (#528687 Global)
9Prior Art Cited
2Claims (0 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A bearing steel consisting of 0.55 to 0.78 percent of carbon, 0.50 to 2.00 percent of chromium, 0.10 to 1.15 percent of manganese and 1.00 to 2.00 percent of silicon by weight with the balance iron, said steel having been spheroidized during annealing, and afterward, heated to an austenitizing temperature ranging from about 810* to 870* C. for a period of about 30 minutes to dissolve 0.35 to 0.55 percent by weight of carbon into austenite retaining 3 to 6 percent by weight of undissolved spheroidized iron carbide, liquid quenched and tempered at about 150* C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 34.

Claims (2 — 0 Independent, 2 Dependent)

  1. Claim 2Depends on #1

    A bearing steel according to claim 1, wherein the carbon is 0.65 to 0.78 percent, and silicon is 1.50 to 1.80 percent by weight.

  2. Claim 3Depends on #2

    A bearing steel according to claim 2, wherein the carbon is 0.65 to 0.70 percent by weight.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Tool Steels, Roberts et al., ASM, 1962, pp. 321 339.