High modulus, low creep strain polyalkene polymer materials
Abstract
Oriented polymer material of high Young's modulus and low creep strain is provided by a process which comprises drawing polymer material having a weight average molecular weight greater than 150,000 and a ratio of weight average molecular weight to number average molecular weight greater than 5 at temperatures from 95 DEG C. to 140 DEG C. and at a rate such that the deformation ratio is greater than 18.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 19.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An oriented polymer material having a weight average molecular weight greater than 300,000; a ratio of weight average molecular weight to number average molecular weight greater than 5; and a creep strain at room temperature of less than 3% after 15 hours under a stress which produces an initial strain of 1% after 10 seconds, said polymer material being selected from the group consisting of ethylene/propylene block copolymers, ethylene/hexene-1-copolymers, polypropylene or a substantially linear polymer of ethylene containing at least 95% by weight of ethylene and having a density from 0.91 to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗