Polymer irradiation
Abstract
A process for the preparation of an oriented homo- or co-polyalkene material of improved strain rate sensitivity, which process comprises subjecting the oriented homo- or co-polyalkene material having a weight average molecular weight (M w )≦350,000, a number average molecular weight (M n )≧5,000, and a 2% secant modulus of at least 10 GPa at a strain rate of 2×10 -5 sec -1 to a high energy irradiation of a dosage of at least 1 Mrad and not more than 60 Mrads at an elevated temperature in vacuo or in an inert or sensitizing atmosphere.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 96.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for the preparation of an oriented homo-polyethylene or co-polyethylene of improved strain rate sensitivity, which process comprises: (1) Providing the solid homo- or copolyethylene; (2) Orienting the molecules of said homo- or co-polyethylene to produce a highly oriented product having a 2% secant modulus of at least 10 GPa at a strain rate of 2×10 -5 sec -1 ; (3) Subjecting the oriented product to a high energy irradiation of a dosage of at least 1 Mrad and not more than 60 Mrads at a temperature of from 30° C. to 140° C. in vacuo or in an inert or sensitizing atmosphere, whe
- Claim 2Depends on #1
A process according to claim 1 wherein the oriented
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 96 total)
References Cited — Backward Prior Art (26)
Non-Patent Literature (5)
- A. Ciferri and I. M. Ward, Ultra High Modulus Polymers, 1979, pp. 322, 323.
- A. Ciferri and I. M. Ward, Ultra-High Modulus Polymers, 1979, pp. 322, 323.
- Chem. Abs. 64 1506e.
- Chem. Abs. 64 19819a.
- Chem. Abs. 66 95721k.