US 4,464,196 A#11142981 Most CitedExpiredUnited States (USPTO)Utility

Acicular ferromagnetic metal particles

9Forward Citations (#11142981 Global)
0.2/yrCitation Velocity (#31978175 Global)
2.95Citation PageRank (#7805174 Global)
15Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Acicular ferromagnetic metal particles consisting essentially of iron and having coercive forces greater than 1300 oersteds when the surface areas of the particles are not greater than 45 m 2 /gram are described. The particles are obtained by reducing a hydrothermally produced α-Fe 2 O 3 with a gaseous reducing agent at a temperature of about 300° to 400° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 9.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Acicular ferromagnetic metallic particles consisting essentially of iron and having an average diameter of 0.03 to 0.1 micron, a length to diameter ratio from about 5/1 to about 13/1, a specific surface area by the BET nitrogen method within the range of 20 to 45 m 2 /gram and a coercivity in oersteds equal to at least the value defined by the equation coercivity=1300+50 (S-20) where S is the specific surface area and is 20 to 30 m 2 /g, or a coercivity greater than 1800 oersteds when the specific surface area is greater than 30 m 2 /g, said coercivity being measured on dry, stable po

  2. Claim 2Depends on #1

    The particles of claim 1 containing from 0.2 to 2% of phosphorus and from 0.5 to 5% cobalt, based on the particle we

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (9 of 9 total)

PatentTitleYearCitations
EP 0,237,943 A3Process for the preparation of acicular alpha-iron-iii oxide—0
EP 0,237,944 A3Process for the preparation of acicular alpha-iron-iii oxide—0
US 2002039667 A1Composite magnetic material and magnetic molding material, magnetic powder compression molding material, and magnetic paint using the composite magnetic material, composite dielectric material and molding material, powder compression molding material, paint, prepreg, and substrate using the composite dielectric material, and electronic part—89
US 7,060,350 B2Composite magnetic material and magnetic molding material, magnetic powder compression molding material, and magnetic paint using the composite magnetic material, composite dielectric material and molding material, powder compression molding material, paint, prepreg, and substrate using the composite dielectric material, and electronic part200641
CN 112,969,544 AMethod for preparing needle-shaped or rod-shaped porous iron powder and needle-shaped or rod-shaped porous iron powder prepared by same—1
US 6,827,758 B2Method for manufacturing magnetic metal powder, and magnetic metal powder20040
US 2005056347 A1Method for manufacturing magnetic metal powder, and magnetic metal powder—20
US 7,416,795 B2Method for manufacturing magnetic metal powder, and magnetic metal powder20080
EP 3,878,580 A4Method for manufacturing needle-shaped or rod-shaped porous iron powder and needle-shaped or rod-shaped porous iron powder manufactured thereby—0

Non-Patent Literature (4)

  • Ferrites: Proceedings of the International Conference, Sep. Oct. 1980, Japan, pp. 633 637.
  • Ferrites: Proceedings of the International Conference, Sep.-Oct. 1980, Japan, pp. 633-637.
  • Magnetic Media Information Services International Newsletter, vol. V, No. 4, Apr. 1982, pp. 64 66. Publication date is not earlier than Aug. 30, 1982.
  • Magnetic Media Information Services International Newsletter, vol. V, No. 4, Apr. 1982, pp. 64-66. Publication date is not earlier than Aug. 30, 1982.