Patents
US 4,133,676 A#12489735 Most CitedExpiredUnited States (USPTO)Utility

Acicular ferromagnetic metal particles and method for preparation of the same

8Forward Citations (#12489735 Global)
0.2/yrCitation Velocity (#35927213 Global)
3.25Citation PageRank (#6646991 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Acicular ferromagnetic metal particles having a particle size of 0.1 to 1 μm and a dimension of crystallite-size of not more than about 215 A in the effective thickness of the crystallite in the direction perpendicular to the reflecting plane (110), which have a high coercive force, preferably not less than 1,400 oersteds and are useful for a high-density magnetic recording tape, video mother tape, or permanent magnet material, and a method for the preparation of the ferromagnetic metal particles comprising reducing with heating goethite particles which are prepared by treating a ferrous salt with a large amount of a basic agent, particularly an alkali metal hydroxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An acicular ferromagnetic metal particle comprising iron element as the essential component, which has a particle size of 0.1 to 1 μm and a dimension of crystallite-size of not more than 215 A in the effective thickness of the crystallite in the direction perpendicular to the reflecting plane (110) (D 110 ).

  2. Claim 2Depends on #1

    The acicular ferromagnetic metal particle according to claim 1, wherein the D 110 is in the range of 140 to 200 A.

  3. Claim 3Depends on #1

    The acicular ferromagnetic metal particle according to claim 1, which has a coercive force of not less than 1,400 oersteds.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗