Patents
US 4,457,797 A#1385263 Most CitedExpiredUnited States (USPTO)Utility

Process for thermoforming reinforced polymer sheets

40Forward Citations (#1385263 Global)
0.9/yrCitation Velocity (#7523900 Global)
7.63Citation PageRank (#1660948 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Reinforced poly(ethylene terephthalate) sheets are thermoformed to articles having one or more surfaces in contact with the mold of such a degree of smoothness that they virtually completely replicate the mold face. When the mold face is completely smooth, the concave imperfections caused by air entrapment in the plastic material account for less than 6% of the surface area. Composite articles consisting of a face member and a backing member are made by thermoforming in a single mold a face member having one or more surfaces in contact with the mold face of such a degree of smoothness that it completely replicates the mold face, and its proportion of concave imperfections is less than about 6% of the surface area. The backing member is bonded in the mold with an adhesive to the face member, and the composite structure is allowed to remain in the mold for a sufficient time to permit subsequent removal without distortion. The initial polymer sheets are less than about 5% crystalline, but the thermoformed article is left in the mold until it crystallizes to the desired degree.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 40.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a process for thermoforming a poly(ethylene terephthalate) sheet having a crystallinity of about 0-5% and a thickness of about 0.76-3.2 mm, which is reinforced with a mineral filler and, when so reinforced, has a tensile modulus at 100° C., defined as average of machine direction and transverse direction, within the range of about 7 to 70 MPa, as determinated according to ASTM D-638, preheated to a temperature of about 80°-130° C., at a draw ratio of less than about 1.8, defined as the ratio of the initial sheet thickness to the minimum wall thickness of the thermoformed article, and at a p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Thermoforming Crystallizing PET, J. L. Throne, Boston, SPE Antec Meeting, 5/5/81, pp. 598 600.
  • Thermoforming Crystallizing PET, J. L. Throne, Boston, SPE-Antec Meeting, 5/5/81, pp. 598-600.