Thermoforming process for polyalkylene terephthalate polyester resins
Abstract
A process for producing shaped articles of polyalkylene terephthalate resins involves thermoforming a substantially unoriented sheet of said resin which sheet has an average crystallinity thermally induced in the range of about 0% to 18% and an average temperature in the range of about 210°-300° F., in contact with a mold at a temperature in the range of about 240°-350° F. which mold is preferably at a higher temperature than said sheet. Optionally a differential in applied pressure below about 5 atmospheres can be utilized in the thermoforming.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 32.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for thermoforming to a draw ratio in excess of about 3 of a polyalkylene terephthalate resin sheet is substantially unoriented, has a half-time for crystallization at 410° F. below about 5 minutes, is at an average temperature in the range of about 210°-300° F., and has an initial thermally induced average crystallinity in the range of about 0% to 18%, said process comprising: (a) contacting said sheet with a deep-draw mold which is at a temperature in the range of about 240°-350° F.; (b) applying forces comprising a differential in applied pressure to said sheet so as to make said
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗