High molecular weight p-polyarylensulfides having a high melt viscosity, capable of being processed thermoplastically, and have good mechanical properties are produced by reacting components (a), (b), and (c) in a polar solvent with a molar ratio of (a):(c) in the range of 0.85:1 to 1.15:1 and a molar ratio of (c): solvent in the range of 1:2 to 1:15, for a time of up to 10 hours at a temperature of from 160° C. to 300° C., and in the presence of from 2 to 100 mole percent, relative to (c), of an N,N-dialkylcarboxamide; wherein component (a) is dihalogenobenzene with 50 to 100 mole percent of the formula ##STR1## and 0 to 50 mole percent of the formula ##STR2## wherein X is fluoro, chloro, bromo or iodo, and R is the same or different and each is selected from the group consisting of hydrogen, alkyl having 1 to 20 carbon atoms, cycloalkyl having 5 to 20 carbon atoms, aryl having 6 to 24 carbon atoms, alkaryl having 7 to 24 carbon atoms, aralkyl having 7 to 24 carbon atoms, and two R moieties linked together forming aryl having 6 to 24 carbon atoms or a heterocyclic moiety having an oxygen, nitrogen or sulphur hetero-atom and having 6 to 24 carbon atoms; with the proviso that at lea

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the process for preparation of high molecular weight thermoplastic branched polyarylene sulphide having a melt viscosity between 0.5×10 3 and 5×10 5 Pa.s by reacting halogenoaromatic compounds with alkali metal sulphides, the improvement comprises reacting components (a), (b) and (c) in a lactam without further metal salt catalyst with a molar ratio of (a):(c) in the range of 0.85:1 to 1.15:1 and a molar ratio of (c): solvent in the range of 1:2 to 1:15, for a time of up to 10 hours at a temperature of from 160° C. to 300° C., and in the presence of from 2 to 100 mole percent, relative to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Patents Abstracts of Japan, vol. 2, No. 76, p. 946C78 (6/16/78).