Abstract
Preparation of a polyarylene sulphide by polycondensing a substituted p-dihalogenobenzene and optionally a polyhalogeno aromatic compound having at least three halo substituents with an alkali metal sulphide in a polar solvent in the presence of a catalytic amount of a di-alkali metal salt of a phosphonic acid.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In the process for preparing a polyarylene sulphide by polycondensing at a temperature of from 160°-285° C. for up to 60 hours (a) a p-dihalogenobenzene which consists of 50-100 mol % of a compound of the formula ##STR4## and 0-50 mol % of a compound of the formula ##STR5## wherein X is fluorine, chlorine, bromine or iodine and each R is independently selected from the group consisting of hydrogen, C 1 -C 20 -alkyl, C 5 -C 20 -cycloalkyl, C 6 -C 24 -aryl, C 7 -C 24 -alkaryl and C 7 -C 24 -aralkyl with the proviso that at least one R is other than hydrogen; and (b) 0-2.0 mol %, base
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,658,753 A | Color stabilized poly(arylene sulfide) resins | 1972 | 20 |