Preparation of amorphous ultra-high-speed-spun polyethylene terephthalate yarn for texturing
Abstract
Spinning of polyethylene terephthalate yarn at speeds in excess of 5000 meters per minute and rapid quenching produces highly oriented, amorphous yarn that gives enhanced bulk on texturing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 26.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for preparing an oriented amorphous polyethylene terephthalate feed yarn for false-twist texturing comprising spinning polyethylene terephthalate at a windup speed of at least 5,000 m./min. and quenching in a room temperature water bath located at a distance from the spinneret such that the quenched filaments have an as-spun boil-off shrinkage of at least 45% and no detectable crystallinity as measured by X-ray diffraction.
- Claim 2Depends on #1
A process according to claim 1 wherein the spun polyethylene terephthalate filaments are quenched in a water bath.
- Claim 3Depends on #1
A process according to claim 1 wherein the polyethylene terephthalate is spun at a windup speed of at least 5,500 m./min.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 26 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (1)
- Journal of Applied Polymer Science, vol. 22, pp. 2229-2243 (1978).