Abstract
The improvement of passing an inert, preferably vaporizable and condensible, liquid material through or over a polyester molten mass in a polymer reactor to further increase surface area-to-volume ratio and/or lower the partial pressure of vaporous products of condensation so that viscosity of the polymer is increased at a substantially greater rate in the same residence time is taught for the prior art condensation process in a film-forming reactor at temperatures of 275 DEG C. to 300 DEG C., pressures of 0.1 to 760 Torr, and residence times of 0.1 to 6 hours. A polymer having an intrinsic viscosity above 0.65, preferably over 0.7, is produced.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 32.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method to increase the reactor capacity and throughput and/or increase final viscosity of the polyester for polycondensation of molten ethylene terephthalate polyesters in a high surface area-to-volume ratio reactor operating at temperatures between about 275° C. and 300° C., pressures between about 0.1 and 760 Torr, and a residence time of between about 0.1 and 6 hours while continuously removing the vaporous products of condensation in a vapor removal system, and increasing the viscosity of the polyester having an initial intrinsic viscosity above 0.4, comprising: a. injecting liquid inert
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 32 total)
References Cited — Backward Prior Art (24)
Non-Patent Literature (2)
- B. V. Petukhon, The Technology of Polyester Fibres, pp. 18 & 19, (1963).
- Jap. Abstract 7210069, 3-72.