Polyester polymers with low acetaldehyde generation rates and high vinyl ends concentration
Abstract
A polyester polymer comprising alkylene arylate units, said polymer having an It.V. of at least 0.72 dl/g, a vinyl ends concentration of at least 0.8 microequivalents per gram, an AA generation rate of less than 20 ppm are prepared by addition of a catalyst deactivator either late in the polycondensation or upon remelting of a solid polyester polymer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for manufacturing a polyester polymer, comprising: a) polycondensing a first polyester polymer in the presence of one or more polycondensation catalysts; b) adding at least one additive compound comprising a catalyst deactivator compound to said first polyester polymer after said first polyester polymer has reached an It.V. of at least 0.68 dl/g, thereby producing the polyester polymer with a vinyl ends concentration of from 0.8 to 2.9 μeg/gram and an AA generation rate at 295° C. for 5 minutes of less than 17.5 ppm, wherein the polyester polymer with a vinyl ends concentration of fr
- Claim 2Depends on #1
The process of claim 1 , wherein the adding b) of said catalyst deactivator compound is after said polyester polymer has reached an It.V. of at least 0.72 dl/g.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.