Abstract
Block copolymers are prepared by heating at above 250° C. (i) a halophenate, (ii) dihalobenzenoid compound plus bisphenate, and/or (iii) a polymer formed from (i) or (ii) having at least one phenate end group, said halophenate and/or dihalobenzenoid compound containing SO 2 groups ortho or para to the halogen atoms, in the presence of a suspension of a crystalline polyetherketone or etherketone/sulphone copolymer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the manufacture of a copolymer whose molecular chains contain phenylene, ketone, and sulphone groups and oxygen atoms comprising heating at a temperature between 250° C. and 300° C., at least one of the reactants selected from (i) at least one alkali metal halophenate containing a sulphone group ortho or para to the halogen atom, (ii) a mixture of a dihalobenzenoid compound containing a sulphone group ortho or para to each halogen atom and a substantially equivalent amount of an alkali metal hydroxide or carbonate, (iii) a mixture of substantially equimolar proportions of at
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗