Aromatic polymers containing ketone linking groups and process for their preparation

43Forward Citations (#1205053 Global)
0.9/yrCitation Velocity (#8127001 Global)
29.98Citation PageRank (#169201 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for the preparation of aromatic polyketones and copolyketone/sulphones (ketone to sulphone content 75/25 to 100/0 having high molecular weight comprises heating dialkali metal salt of a bisphenol containing ketone linking groups with equimolar or slight molar excess of dihalobenzenoid compound having halogen atoms activated by a ketone or sulphone linking group in the presence of certain diaryl sulphones at 250° to 400° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 43.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of aromatic polymers having reduced viscosity of between 0.8 and 3.0, as measured at 25° C on a solution of polymer in concentrated sulphuric acid of density 1.84 g/cm 3 containing 1 g of polymer in 100 cm 3 of solution, which comprises heating at a temperature of 250° to 400° C a monomer mixture comprising 1. 49 to 50% molar of a di(alkali metal) salt of at least one bisphenol of the formula ##STR21## at least 95% of the phenolic OH groups being in the para position, and 2. 51 to 50% molar at least one dihalo compound of the formula ##STR22## where Q is SO 2

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗