Methods of producing silicon steel strip
Abstract
A method of producing silicon steel strip from slabs is provided which includes the steps of reducing the slabs in a planetary mill to a thickness of 0.060 to 0.10 inch at a temperature above that at which MnS will precipitate, cooling to between 800 DEG F. to 1500 DEG F. and reducing the strip at that temperature to a thickness of 0.020 to 0.030.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 6.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
The method of producing silicon steel strip for magnetic purposes from slabs comprising the steps of: (a) heating the slabs to a temperature above 2200° F., to stabilize MnS, and immediately rolling said slabs into strip in a planetary mill of the Zendzimer type to a thickness range of about 0.060 to 0.150 inch while maintaining the temperature in the temperature range 2100° F. to 2200° F., during said rolling, and (b) quenching the strip to precipitate MnS.
- Claim 2Independent Claim
The method of producing silicon steel strip for magnetic purposes from slabs comprising the steps of: (a) heating the slabs to a temperature above 2200° F., to stabilize MnS, and immediately rolling said slabs into strip in a planetary mill of the Platzer type to a thickness range of about 0.060 to 0.150 inch while maintaining the temperature in the temperature range 2100° F. to 22
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (1)
- McGannon, H.; Making, Shaping and Treating of Steel, Pittsburgh, (U.S. Steel), 1964, pp. 571-573.