US 3,969,162 A#10930868 Most CitedExpiredUnited States (USPTO)Utility

Method of producing silicon steel strip

9Forward Citations (#10930868 Global)
0.2/yrCitation Velocity (#34985292 Global)
7.16Citation PageRank (#1845753 Global)
7Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of producing silicon steel strip from slabs is provided which includes the steps of reducing the slabs in a planetary mill to a thickness of 0.060 to 0.10 inch at a temperature above that at which MnS will precipitate, cooling to between 300°F to 1500°F and reducing the strip at that temperature to a thickness of 0.020 to 0.030.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 9.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    The method of producing oriented silicon steel strip of improved physical properties having a silicon content in the range 2.5 to 4.0 percent comprising the steps of: a. bringing hot rolled strip having a thickness in the range 0.060 to 0.150 inch following normalizing to a temperature below 1500°F. and above 600°F., b. reducing the strip in thickness to final finish thickness prior to recrystallize normalizing to about 0.020 to 0.030 inch while in said temperature range 600°F. to 1500°F., c. normalizing at about 1725°F. to recrystallize grain strength, and d. cold rolling to a selected

  2. Claim 2Depends on #1

    The method of producing silicon steel strip as claimed in claim 1 wherein the strip is reduced to about 0.026 inch while in the range 600°F. to 1500°F.

  3. Claim 3Independent Claim

    The method of producing silicon steel s