Processing for electromagnetic silicon steel
Abstract
A process for producing electromagnetic silicon steel having a cube-on-edge orientation. The process includes the steps of: preparing a melt of silicon steel having up to 0.07% carbon, from 0.01 to 0.25% manganese, from 0.01 to 0.09% of material from the group consisting of sulfur and selenium, from 2.5 to 4.0% silicon, up to 1.0% copper, less than 0.009% aluminum and less than 0.0006% boron; casting the steel; hot rolling the steel; cold rolling the steel; normalizing the steel in a hydrogen-bearing atmosphere having a pH 2 O/pH 2 of from 0.015 to 0.3; applying a refractory oxide coating containing an oxide less stable than SiO 2 at temperatures up to 2150° F.; and final texture annealing the steel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a process for producing electromagnetic silicon steel having a cube-on-edge orientation, which process includes the steps of: preparing a melt of silicon steel having up to 0.07% carbon, from 0.01 to 0.25% manganese, from 0.01 to 0.09% of material from the group consisting of sulfur and selenium, from 2.5 to 4.0% silicon, up to 1.0% copper, less than 0.009% aluminum and less than 0.0006% boron; casting said steel; hot rolling said steel; cold rolling said steel; decarburizing said steel; annealing said cold roll steel of final gage; applying a refractory oxide coating to said steel; and fin
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗