Abstract
A process for producing electromagnetic silicon steel having a cube-on-edge orientation and a permeability of at least 1870 (G/O e ) at 10 oersteds. The process includes the steps of: preparing a melt of silicon steel containing from 0.02 to 0.06% carbon, from 0.0006 to 0.0080% boron, up to 0.0100% nitrogen, no more than 0.008% aluminum and from 2.5 to 4.0% silicon; casting said steel; hot rolling said steel; cold rolling said steel to a thickness no greater than 0.020 inch; decarburizing said steel to a carbon level below 0.005%; normalizing said steel at a temperature of from 1550° to 2000° F in a hydrogen-bearing atmosphere; applying a refractory oxide base coating to said steel; and final texture annealing said steel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 14.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a process for producing electromagnetic silicon steel having a cube-on-edge orientation and a permeability of at least 1870 (G/O e ) at 10 oersteds, which process includes the steps of: preparing a melt of silicon steel containing from 0.02 to 0.06% carbon, from 0.015 to 0.15% manganese, from 0.01 to 0.05% of material from the group consisting of sulfur and selenium, from 0.0006 to 0.0080% boron, up to 0.0100% nitrogen, up to 1.0% copper, no more than 0.008% aluminum and from 2.5 to 4.0% silicon; casting said steel; hot rolling said steel; cold rolling said steel to a final gage no greater
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗