Lead-free glass material for organic-el sealing, organic el display formed using the same
Abstract
A lead-free glass material for sealing organic EL elements is provided with which satisfactory sealing quality is obtained through laser sealing without requiring the addition of a metallic powder. The lead-free glass material for sealing organic EL elements has a glass composition which comprises, in terms of mol %, 30-60% V 2 O 5 , 5-20% ZnO, 5-20% BaO, 15-40% TeO 2 , 0-7% Nb 2 O 5 , 0-7% Al 2 O 3 , 0-5% SiO 2 , 0-5% MgO, 0-5% Sb 2 O 3 , 0-4% CuO, and 0-4% SnO and in which Nb 2 O 5 +Al 2 O 3 is 0.5-10%, SiO 2 +MgO+Sb 2 O 3 is 0-5%, and CuO+SnO is 0-4%. The glass material has low-temperature softening properties, melt stability, and a low coefficient of thermal expansion and is inhibited from thermally adversely affecting organic EL elements The glass material can attain high sealing properties and high sealing strength in high yield.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 14.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2009247385 A1 | Frit | — | 38 |