US 10,913,680 B2#31047075 Most CitedActiveUnited States (USPTO)Utility

Lead-free glass composition, glass composite material, glass paste, sealing structure, electrical/electronic component and coated component

3Forward Citations (#31047075 Global)
0.6/yrCitation Velocity (#13294210 Global)
1.18Citation PageRank (#33181568 Global)
16Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The purpose of the present invention is to provide a lead-free glass composition in which crystallization is suppressed and which has a low softening point. This lead-free glass composition is characterized by containing silver oxide, tellurium oxide and vanadium oxide, and further containing at least one compound selected from among yttrium oxide, lanthanum oxide, cerium oxide, erbium oxide, ytterbium oxide, aluminum oxide, gallium oxide, indium oxide, iron oxide, tungsten oxide and molybdenum oxide as an additional component, and in that the content values (mol %) of silver oxide, tellurium oxide and vanadium oxide satisfy the relationships Ag2O>TeO2≥V2O5 and Ag5O≤2V2O5 when calculated in terms of the oxides, and in that the content of TeO2 is 25-37 mol. %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A lead-free glass composition, containing silver oxide, tellurium oxide, and vanadium oxide, further, as additional components, containing at least one of yttrium oxide, lanthanum oxide, cerium oxide, erbium oxide, ytterbium oxide, aluminum oxide, gallium oxide, indium oxide, and iron oxide, wherein the contents (mol %) of the silver oxide, the tellurium oxide, and the vanadium oxide, when calculated in terms of the oxides as shown below, have the relationship of Ag 2 O>TeO 2 ≥V 2 O 5 , and Ag 2 O≤2V 2 O 5 , and wherein the content of TeO 2 is 25 mol % to 37 mol %.

  2. Claim 2Depends on #1

    The lead-free glass composition according to claim 1 , wherein, when calculated in terms of the oxides, the content of Ag 2 O is equal to or greater than 40 mol % and less than 50 mol %, and the content of V 2 O 5 is equal to or greater than 20 mol

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
US 5,334,558 ALow temperature glass with improved thermal stress properties and method of use199450
JP H08502468 A改良された熱応力特性を有する低温ガラスおよびその使用方法—39
US 2012321902 A1Lead-free glass material for organic-el sealing, organic el display formed using the same—14
JP 2013032255 AGlass composition, glass frit including the same, glass paste including the same, and electric electronic component using the same—47
JP 2013133342 AComposite material—6
JP 2013132756 ALaminate and organic el element using the same, and window and solar cell module—6
WO 2014/073086 A1Bonded structure and production method therefor—5
US 2014145122 A1Glass composition, glass frit containing same, glass paste containing same, and electrical/electronic component obtained using same—50
US 2014334937 A1Composite material—2
US 2015020879 A1Laminate and organic el element, window, and solar battery module using same—2
US 2015279700 A1Bonded Structure and Production Method Therefor—8
US 2016060158 A1Lead-free low-melting glass composition, low-temperature sealing glass frit, low-temperature sealing glass paste, conductive material, and conductive glass paste containing glass composition, and glass-sealed component and electric/electronic component prepared using the same—12
US 2016229737 A1Lead-free low-melting glass composition, low-temperature sealing glass frit, low-temperature sealing glass paste, conductive material, and conductive glass paste containing glass composition, and glass-sealed component and electric/electronic component prepared using the same—7
US 9,815,735 B2Lead-free glass and sealing material20175
US 9,824,900 B2Bonded structure and production method therefor20173
US 10,252,938 B2Glass composition, glass frit containing same, glass paste containing same, and electrical/electronic component obtained using same20195