hottub.patents
US 12,674,052 B2#3199335 Most CitedActiveUnited States (USPTO)Utility

Polypropylene composition for cable insulation

0Forward Citations (#3199335 Global)
0.0/yrCitation Velocity (#3199335 Global)
0.00Citation PageRank (#3199335 Global)
52Prior Art Cited
15Claims (1 Indep. · 14 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a cable comprising at least one layer comprising a polypropylene composition comprising (A) from 80.0 to 99.0 wt.-%, preferably from 82.5 to 97.2 wt. %, most preferably from 85.0 to 95.0 wt.-% of a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms having a total amount of comonomer units of from 10.0 to 16.0 wt %, preferably from 11.0 to 15.0 wt %, most preferably from 12.0 to 14.0 wt %, based on the total amount of monomer units of the copolymer of propylene (A); a melt flow rate MFR2 of from 0.5 to 2.5 g/10 min, preferably from 0.8 to 2.3 g/10 min, still more preferably from 1.0 to 2.0 g/10 min and most preferably from 1.2 to 1.7 g/10 min; a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, preferably from 27.5 to 45.0 wt %, more preferably from 30.0 to 42.5 wt % and most preferably from 32.5 to 40.0 wt %, based on the total weight amount of the copolymer of propylene (A); and (B) from 1.0 to 20.0 wt.-%, preferably from 2.5 to 17.5 wt %, most preferably from 5.0 to 15.0 wt.-% of a propylene polymer having a density of from 855 to 890 kg/m, preferably from 860 to 885 kg/m 3 , mot preferably from 865 to 880 kg/m 3 .

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 52 · Forward citations: 0.

Claims (15 — 1 Independent, 14 Dependent)

  1. Claim 1Independent Claim

    A cable comprising at least one layer comprising a polypropylene composition comprising: (A) from 80.0 to 99.0 wt.-%, based on the total weight of the polypropylene composition, of a copolymer of propylene and comonomer units selected from ethylene and alpha-olefins having from 4 to 12 carbon atoms having a total amount of comonomer units of from 10.0 to 16.0 wt %, based on the total amount of monomer units of the copolymer of propylene (A), determined by quantitative 13 C{ 1 H} NMR measurement; a melt flow rate MFR 2 of from 0.5 to 2.5 g/10 min, determined according to ISO 1133 at 230 ° C. and 2.16 kg; a xylene cold soluble (XCS) fraction in a total amount of from 25.0 to 50.0 wt %, based on the total weight amount of the copolymer of propylene (A) and determined according to ISO16152; and (B) from 1.0 to 20.0 wt.-%, based on the total weight of the polypropylene composition, of a propylene polymer having a density of from 855 to 890 kg/m 3, determined according to ISO 1183 or ASTM D 792, wherein the polypropylene composition has an intrinsic viscosity of the xylene cold soluble (XCS) fraction of from 150 to 240 cm 3 /g, measured in decalin, a glass temperature attributed to a matrix phase Tg (matrix) in the range of from − 1.0 to − 17.5 ° C. and a glass temperature attributed to an elastomeric phase Tg (EP) of from − 40.0 to − 55.0 ° C., both determined by dynamic mechanical analysis.

  2. Claim 2Depends on #1

    The cable according to claim 1, wherein the copolymer of propylene (A) is a heterophasic copolymer of propylene which comprises a matrix phase and an elastomeric phase dispersed in said matrix phase, which preferably comprises two glass transition temperatures attributed to the matrix phase and the elastomeric phase, wherein the glass transition temperature attributed to the matrix phase Tg (matrix) is in the range of from − 1.0 to − 15.0 ° C. and/or the glass transition temperature attributed to the elastomeric phase Tg (EP) is in the range of from − 40.0 to − 55.0 ° C., wherein Tg (matrix) and Tg (EP) are determined by dynamic mechanical analysis.

  3. Claim 3Depends on #1

    The cable according to claim 1, wherein xylene cold soluble (XCS) fraction of the copolymer of propylene (A) has an amount of comonomer units, preferably of ethylene, of from 23.0 to 35.0 wt %, based on the total amount of monomer units in the xylene cold soluble (XCS) fraction and determined by quantitative 13 C{ 1 H} NMR measurement and/or an intrinsic viscosity of from 150 to 350 cm 3 /g, measured in decalin according to ISO 1628-3; and/or the copolymer of propylene (A) has a fraction insoluble in cold xylene (XCI) in a total amount of from 50.0 to 75.0 wt %, based on the total weight amount of the copolymer of propylene (A) and determined according to ISO16152, and wherein the fraction insoluble in cold xylene (XCI) preferably has an amount of comonomer units, preferably of ethylene, of from 3.0 to 9.0 wt %, based on the total amount of monomer units in the fraction insoluble in cold xylene (XCI) and determined by quantitative 13 C{ 1 H} NMR measurement and/or an intrinsic viscosity of preferably from 185 to 350 cm 3 /g, measured in decalin according to ISO 1628-3.

  4. Claim 4Depends on #1

    The cable according to claim 1, wherein the copolymer of propylene (A) has one or more or all of the following properties: a flexural modulus of from 130 MPa to 400 MPa, determined according to ISO 178 method A; and/or a Charpy notched impact strength at 23 ° C. of from 50 to 110 kJ/m 2, determined according to ISO 179-1/1 eA; and/or a Charpy notched impact strength at − 20 ° C. of from 5.0 to 10.0 kJ/m 2, determined according to ISO 179-1/1 eA.

  5. Claim 5Depends on #1

    The cable according to claim 1, wherein the propylene polymer (B) is a propylene homopolymer, an elastomeric copolymer of propylene and ethylene or a wax of copolymer of propylene and ethylene.

  6. Claim 6Depends on #1

    The cable according to claim 1, wherein the propylene polymer (B) is a propylene homopolymer having one or more or all of the following properties: a melt flow rate MFR 2 of from 500 to 5000 g/10 min, determined according to ISO 1133 at 230 ° C. and 2.16 kg; and/or a melting temperature Tm of from 65 to 95 ° C., determined by differential scanning calorimetry; and/or a weight average molecular weight Mw of from 20 to 100 kg/mol, measurable by GPC; and/or a viscosity at 190 ° C. of from 1000 to 50000 mPas; and/or a tensile modulus of from 25 to 150 MPa, measurable by ISO 527-1.

  7. Claim 7Depends on #1

    The cable according to claim 1, wherein the propylene polymer (B) is an elastomeric copolymer of propylene and ethylene having one or more or all of the following properties: a melt flow rate MFR 2 of from 5000 to 50000 g/10 min, determined according to ISO 1133 at 230 ° C. and 2.16 kg; and/or a melting temperature Tm of from 80 to 110 ° C., determined by differential scanning calorimetry; and/or a glass transition temperature Tg of from − 40 to − 10 ° C., determined by dynamic mechanical analysis; and/or a viscosity at 190 ° C. of from 500 to 10000 mPas; and/or an ethylene content of from 2.5 to 10.0 wt.-%, measurable using quantitative nuclear-magnetic resonance (NMR) spectroscopy.

  8. Claim 8Depends on #1

    The cable according to claim 1, wherein the propylene polymer (B) is an elastomeric copolymer propylene and ethylene having one or more or all of the following properties: a melt flow rate MFR 2 of from 5.0 to 100 g/10 min, determined according to ISO 1133 at 230 ° C. and 2.16 kg; and/or a melting temperature Tm of from 50 to 95 ° C., determined by differential scanning calorimetry; and/or a glass transition temperature Tg of from − 40 to − 10 ° C., determined by dynamic mechanical analysis; and/or a crystallinity of from 5 to 50%; and/or a flexural modulus of from 15 to 200 MPa, determined according to ISO 178 method A.

  9. Claim 9Depends on #1

    The cable according to claim 1, wherein the propylene polymer (B) is wax of copolymer propylene and ethylene having one or more or all of the following properties: a melt viscosity at 170 ° C. of from 50 to 500 mPas; and/or a melting temperature Tm of from 65 to 95 ° C., determined by differential scanning calorimetry; and/or a crystallization temperature Tc of from 25 to 55 ° C., determined by differential scanning calorimetry; and/or a drop point of from 75 to 105 ° C., measurable according to ASTM D 3954.

  10. Claim 10Depends on #1

    The cable according to claim 1, wherein the polypropylene composition has one or more or all of the following properties: a melt flow rate MFR 2 of 0.5 to 3.5 g/10 min, determined according to ISO 1133 at 230 ° C. and 2.16 kg; and/or a melting temperature Tm of from 140 to 159 ° C., determined by differential scanning calorimetry; and/or a crystallization temperature Tc of from 85 to 130 ° C., determined by differential scanning calorimetry; and/or a difference of the melting temperature to the crystallization temperature Tm-Tc is in the range of from 20 to 65 ° C.; and/or shear thinning index SHI 1/100 of from 2.5 to 22.5, determined by dynamic shear measurements; and/or a polydispersity index PI of from 1.0 to 4.5 s − 1, determined by dynamic shear measurements.

  11. Claim 11Depends on #1

    The cable according to claim 1, wherein the polypropylene composition has one or more or all of the following properties: a flexural modulus of from 150 MPa to 450 Mpa, determined according to ISO 178 method A; and/or a Charpy notched impact strength at 23 ° C. of from 50 to 110 KJ/m 2, determined according to ISO 179-1/1 eA; and/or a Charpy notched impact strength at − 20 ° C. of from 1.5 to 25.0 kJ/m 2, determined according to ISO 179-1/1 eA.

  12. Claim 12Depends on #1

    The cable according to claim 1, wherein the polypropylene composition is free of a dielectric fluid.

  13. Claim 13Depends on #1

    The cable according to claim 1, wherein the at least one layer is an insulation layer.

  14. Claim 14Depends on #1

    The cable according to claim 1 being a medium voltage cable or high voltage cable, comprising an insulation layer comprising the polypropylene composition.

  15. Claim 15Depends on #1

    The cable according to claim 1 having a Weibull alpha-value of from 35.0 to 65.0 kV/mm and/or a Weibull beta-value of from 5.0 to 250.0, measured on a 10 kV cable in agreement with CENELEC HD 605 5.4.15.3.4 for 6/10 kV cables.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATION(S) The present application is a national stage entry under 35 U.S.C. § 371 of International Application No. PCT/EP2023/076455, filed on Sep. 26, 2023, which claims priority to European (EP) patent application Ser. No. 22/198,327.3, filed on Sep. 28, 2022. The contents of these applications are hereby incorporated by reference in their entirety. FIELD OF THE INVENTION The present invention relates to a cable comprising an insulation layer comprising a flexible polypropylene composition. TECHNICAL BACKGROUND Nowadays, ethylene polymer products are used as insulation and semiconducting shields for low, medium and high voltage cables, due to easy processability and their beneficial electrical properties. In addition, in low voltage applications polyvinyl chloride (PVC) is also commonly used as insulation material, usually in combination with softeners to reach desirable softness of cables. PVC is a thermoplastic which by incorporation of various plasticizers can be used in a wide temperature range. For standard PVC a continuous conductor temperature of max. 70 ° C. is normal. At low temperatures PVC becomes rigid and usage temperatures below − 10 ° C. should be avoided. At conductor temperatures over 100 ° C. the plasticizers migrate out and the materials lose their flexibility. However, with the addition of special plasticizers and stabilizers, PVC materials can be produced for conductor temperatures of 90-105 ° C. But in essence, PVC is mainly used for the 1 kV area, as the higher permittivity and dissipation factor of the material means that the losses increase too much at higher voltages and therefore PVC cables are not normally not used over 1 kV. In addition, softeners have to be added to PVC in order to maintain a high level of flexibility. Insufficient amounts of softeners reduce low temperature properties of PVC significantly. From an environmental point of view, these softeners are not always regarded as problem-free, mak

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (52)

PatentTitleYearCitations
US 5,234,879 AMethod for the modification of catalysts intended for the polymerization of olefins1993128
US 8,680,207 B2Heterophasic polypropylene resin20144
US 8,901,249 B2Composition based on polypropylene compounds with styrenic based elastomers20140
US 9,296,884 B2Propylene polymer compositions20160
US 9,890,274 B2Heterophasic polypropylene with improved impact strength/stiffness balance, improved powder flowability, reduced emissions and low shrinkage20184
US 10,385,196 B2Polypropylene films with improved printability20194
US 10,781,304 B2Polypropylene compositions with low fogging20200
US 10,800,910 B2High flow heterophasic polypropylene copolymers with improved mechanical and optical properties20201
US 11,292,858 B2Polypropylene composition combining low sealing initiation temperature and high melting temperature20224
US 11,384,232 B2Heterophasic propylene polymerization material20220
US 11,578,198 B2Polypropylene composition with low shrinkage at wide application temperature range20231
KR 20220135779 AReturnable box—1
CN 111,630,077 APolypropylene resin for wire insulation—1
EA 033,422 B1Heterophasic polypropylene composition with improved impact strength/stiffness balance, improved powder flowability, reduced emission and low shrinkage, process for preparation and use thereof—0
EA 038,637 B1Novel polypropylene compositions with low fogging—0
EP 0,491,566 A2A method for the modification of catalysts intended for the polymerization of olefins—345
EP 0,586,390 B1Coarse grained polyolefin, production thereof and a procatalyst containing a transesterification product between a lower alcohol and dioctylphthalate used therefore199740
EP 0,591,224 B1A procatalyst for polymerization of olefins containing a trans-esterification product of a lower alcohol and a phthalic acid ester199855
EP 0,887,379 B1Process and apparatus for preparing propylene homopolymers and copolymers200431
EP 1,681,315 A1Heterophasic polymer composition and process for its preparation—46
EP 2,739,679 A1Energy cable having a thermoplastic electrically insulating layer—12
EP 3,741,806 A1Polyolefin resin composition for electric wire insulation—1
KR 20120061980 AHeterophasic polypropylene resin—4
KR 101,985,611 B1Polyolefin Resin Composition for Insulating Power Cables201911
RU 2,478,668 C2Composition based on polypropylene with styrene-based elastomers20135
RU 2,528,384 C2Propylene polymer-based compositions20141
RU 2,712,913 C1Polypropylene films with improved suitability for printing20200
RU 2,724,050 C1Polypropylene-based composition having low welding start temperature and high melting point20200

Non-Patent Literature (10)

  • Translation of CN111630077 obtained by the European Patent Office in November of 2025 (Year: 2020).
  • International Search Report and Written Opinion for Patent Application No. PCT/EP2023/076455 mailed Dec. 20, 2023, 11 pages.
  • European Search Report for European Patent Application No. 22198327.3 dated Feb. 27, 2023, 6 pages.
  • Busico, et al.,
  • “
  • Microstructure of polypropylene,
  • ”
  • Progress in Polymer Science, vol. 26, 2001, pp. 443-533.
  • Busico, et al.,
  • “