Heterophasic polypropylene resin
Abstract
Heterophasic polypropylene resin comprising a propylene random copolymer matrix phase (A), and an ethylene-propylene copolymer rubber phase (B) dispersed within the matrix phase wherein the heterophasic polypropylene resin has a MFR (2.16 kg, 230° C.) of 1.0 to 100 g/10 min, determined according to ISO 1133, and a fraction soluble in p-xylene at 25° C. (XCS fraction) which is present in the resin in an amount of 28 to 50 wt %, and which has a molecular weight distribution (M w /M n ) of 1.0 to 4.0.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 4.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
Heterophasic polypropylene resin comprising a propylene random copolymer matrix phase (A), and an ethylene-propylene copolymer rubber phase (B) dispersed within the matrix phase wherein the heterophasic polypropylene resin has a MFR (2.16 kg, 230° C.) of 1.0 to 100 g/10 min, determined according to ISO 1133, and a fraction soluble in p-xylene at 25° C. (XCS fraction) which is present in the resin in an amount of 28 to 50 wt %, and which has a molecular weight distribution (M w /M n ) of 1.0 to 4.0, and which has an amount of ethylene comonomer units of 10 to 25 wt %.
- Claim 2Depends on #1
The heterophasic polypropylene resin according to claim 1 , wherein the matrix phase (A) has a comonomer content of 0.1 to 4.5 wt %, and wherein the comonomer units in matrix phase (A) are selected from a group consisting of alpha-olefins having 2 an
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (1)
- International Search Report and Written Opinion for International Application No. PCT/EP2010/006449.