Patents
EP 0,018,445 A1#5101159 Most Cited · 17 citations0.4/yr · PR 7.31PendingEP · Application
Process for the manufacture of castings of nodular castiron

1. Method of producing castings from cast iron with spheroidal graphite with a mixed austenitic-bainitic mixed structure from a melt with the usual amounts of silicon, carbon, phosphorus, sulphur and magnesium and also additional amounts of manganese, molybdenum, possibly copper…

US 3,976,474 A#16568937 Most Cited · 6 citations0.1/yr · PR 2.38ExpiredUS · Utility
Covering layer for metallic baths
Inventors: Wunder Wolf, Kohne Volker, Hill Rosolde, Leogrande AntonioAssignee: Ver Deutsche Metallwerke AgFiled 1975-05-19 · Granted 1976-08-24

A covering layer for metallic baths, i.e. baths of molten metal or metal alloys, especially brass or brass-forming compositions consisting of premelted homogeneous finely divided alkali borosilicate glass in a particle size of less than 60 microns and a composition of…

DE 2,245,902 A1#19372435 Most Cited · 5 citations0.1/yr · PR 2.18PendingDE · Application
Spheroidal graphite cast iron prodn. - by adding magnesium carriers, treat-ment with oxygen, and inoculation
Inventors: Wunder Wolf Dipl Ing DrAssignee: Schmidt Gmbh KarlFiled 1972-09-19

Mg carrier-treated cast iron melts are admixed with a measured amount of O2, esp. 0.001-0.5 (0.05-0.5) 1/kg and then inoculated in standard manner, e.g. with FeSi, O2 is pref. supplied pure, as air or as O2-carriers, e.g. roll scale, Fe2O3 or MnO2; through a lance, porous…

DE 2,540,142 A1#26527883 Most Cited · 4 citations0.1/yr · PR 1.19PendingDE · Application
Immersion bell for treating molten iron - esp. with magnesium to mfr. nodular graphite cast iron

Device for the treatment of molten metals, esp. iron alloys, with metal which are volatile at the treatment temp. esp. Mg or the alkali metals uses a bell which is immersed in the melt with its open end downwards. Inside the bell is a crucible which is free to move about in the…

DE 2,246,723 B1#29773934 Most Cited · 3 citations0.1/yr · PR 1.27ExpiredDE · Utility
Non ferrous melt surface protection - using a glass compsn

The glassy material is composed of ground alkali-borosilicate glass of 60 mu particle size. The premolten glass of compsn. 30-38% Na2O, 12-65% B2O3, 5-60% SiO2 has a softening pt. 850 degrees C. and good wetting props. Esp. suitable for Cu alloy metls e.g. brasses.

CA 1,164,777 A#34523413 Most Cited · 2 citations0.1/yr · PR 1.77ExpiredCA · Utility
Cast iron with spheroidal graphite with austenitic- bainitic mixed structure
Inventors: Muehlberger Horst, Prinz Bruno, Wunder Wolf, Schaefer Ulrich, Bognar JosefAssignee: Muehlberger Horst, Prinz BrunoFiled 1980-06-12 · Granted 1984-04-03

ABSTRACT OF THE DISCLOSURE: A process for the production of spheroidal graphite cast iron with an austenitic-bainitic structure. In this process, a cast iron containing up to 0.3 % of manganese and from 0.2 to 0.8 % of molybdenum is subjected to an austenitic heat treatment at a…

DE 2,323,073 A1#39818421 Most Cited · 2 citations0.0/yr · PR 1.02PendingDE · Application
Ground glass frit for covering molten metal - to protect against oxidation during melting

Glass of compsn. 10-70% B2O3, 5-65% SiO2 and 5-40% Na2O, K2O and/or Li2O is used as an oxidation protective cover for molten metals such as brass. The glass has a low m.pt. so that its viscosity is low at the working temp. hence it flows freely over the surface of the melt…

DE 2,416,141 A1#35306068 Most Cited · 2 citations0.0/yr · PR 1.36PendingDE · Application
Sheet metal mould - for the continuous casting of aluminium strip

The strip mould for the continuous casting of Al strip or sheet is made of a material which has no thermal expansion, or only a very small expansion in the range of the operating temp. of the mould. It is made of an alloy contg. 30-40%. pref. 34-38% Ni, balance Fe and usual…

DE 2,444,269 A1#36652051 Most Cited · 2 citations0.0/yr · PR 1.15PendingDE · Application
Segregation- free band shaped, cast strands mfr on band casting mach - where a melt in caused to solidify between revolving casting belts

In mfr. of segregation-free, band-shaped cast strands on band-(strip-) casting machines, the melt is caused to solidify between moving casting belts or the like. In the shrink gap, formed between cast strand and casting belt, heat transfer conditions are maintained such that at…

DE 2,853,871 A1#35465908 Most Cited · 2 citations0.0/yr · PR 1.32PendingDE · Application
Heat treatment of cast iron, esp. nodular cast iron - where controlled cooling results in mechanical properties comparable with those of steel

The iron is heated for 1/4.-5 hr., esp. for 15-40 mins. at min. 730 degrees C, esp. at 730-920 degrees C; and is then cooled in less than 20 mins. to max. 600 degrees C, esp. to 300-600 degrees C in a heated bath. In the case of nodular cast iron, the pref. treatment consists of…

DE 2,419,452 A1#144301881 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Protective layer for steel continuous casting belts - comprising water glass and muscovite-sodium silico fluoride mixture added to inorganic layer

A continuous casting machine for aluminium and aluminium alloys, using steel belts under tension for the casting chamber, uses a special protective coating on the belts. The coating is made from a mixt. of 2-3 pts. wt. water glass and 1 pt. finely powdered muscovite and sodium…

DE 2,446,491 A1#143215952 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Protective layers for metallic casting strands - applied from mixt. of powdered refractory filler, alkali silicate soln and chemical hardener

The patent patent discloses a protective layer, consisting of a mixt of mica and Na silico-fluorite with water glass, for metallic pouring conveyors of a casting machine. According to present patent the protective layer consists of a mixt. of a powdered, refractory filler, an…

DE 2,904,334 A1#98305333 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Low temp. heat treated spheroidal graphite cast iron - is given pearlite-sorbite structure by austenising treatment

Spheroidal graphite cast iron having a ferritic structure is given a pearlitic-sorbitic structure by applying an austentistic heat treatment at 760-910 degrees C (820-840 degrees C) using a holding time of 10-60 min. (20-40 min.). The cast iron is subsequently cooled in moving…