The aluminum alloy has 9-11.5wt.% silicon, 0.45-0.8wt.% manganese, 0.2-1.0wt.% magnesium, 0.1-1.0wt.% copper, not > 0.2wt.% zinc, not > 0.4wt.% zirconium, not > 0.4wt.% chromium, not > 0.3wt.% molybdenum, not > 0.2wt.% iron, not > 0.15wt% titanium,…
Wiesner Stuart
Aluminum alloy comprises 9-11.5 wt.% of silicon, 0.5-0.8 wt.% of manganese, 0.2-1 wt.% of magnesium, 0.1-1 wt.% of copper, 0.2-1.5 wt.% of zinc, 0.05-0.4 wt.% of zirconium, 0.01-0.4 wt.% of chromium, maximum 0.2 wt.% of iron, maximum 0.15 wt.% of titanium, 0.01-0.02% wt.% of…
Aluminium alloy for components having increased strength with a yield point Rp 0.2 >120 MPa and at the same time an elongation at break A>7% in the cast state, a yield point Rp 0.2 >200 MPa and at the same time an elongation at break A>6% after a T5 heat treatment or…
An aluminium alloy for components with increased rigidity, having a tensile yield strength Rp0.2>200 MPa and simultaneous elongation at break A; 6% after a heat treatment, or a tensile yield strength Rp 0.2>120 MPa and simultaneously high elongation at break A>9 % in…
The present invention relates to a kind of aluminium-silicon substrate diecasting alloys, consist of the following compositions: the silicon of 8.5 to 11.5 weight %, the magnesium of 0.1 to 0.5 weight %, the manganese of 0.3 to 0.8 weight %, the iron of 0.02 to 0.5 weight %, the…
The present invention relates to a kind of casting alloys, it includes following substances: a kind of element or one group of element for being selected from chromium, nickel, molybdenum, zirconium, vanadium, hafnium, calcium, gallium and boron of iron 0.8-3.0 weight %,…
The invention relates to an aluminum, magnesium and silicon-based die-casting alloy which is composed of the following substances: 5.0-7.0 wt.% magnesium, 1.5-7.0 wt.% silicon, 0.3-0.8 wt.% manganese, 0.03-0.5 wt.% iron, 0.01-0.4 wt.% molybdenum, 0.01-0.3 wt.% zirconium, 0-0.25…
A die casting alloy on an aluminum-silicon base with a composition having 8.5 to 11.5 wt. % of silicon, 0.1 to 0.5 wt. % of magnesium, 0.3 to 0.8 wt. % of manganese, 0.02 to 0.5 wt. % of iron, 0.005 to 0.5 wt. % of zinc, 0.1 to 0.5 wt. % of copper, 0.02 to 0.3 wt. % of…
An aluminum alloy for components with increased rigidity, having a tensile yield strength Rp0.2>200 MPa and simultaneous elongation at break A>6% after a heat treatment, or a tensile yield strength Rp 0.2>120 MPa and simultaneously high elongation at break A>9% in…
A cast alloy including iron 0.8-3.0 wt. %, magnesium 0.01-9.0 wt. %, manganese 0-2.5 wt. %, beryllium 0-500 ppm, titanium 0-0.5 wt. %, silicon 0-0.8 wt. %, strontium 0-0.8 wt. %, phosphorus 0-500 ppm, copper 0-4 wt. %, zinc 0-10 wt. %, 0-0.5 wt. % of an element or a group of…
본 발명은, 다음으로 구성되는, 알루미늄, 마그네슘 및 규소 기재의 다이 캐스팅 합금에 관한 것으로: 5.0 내지 7.0 중량 % 마그네슘; 1.5 내지 7.0 중량 % 규소; 0.3 내지 0.8 중량 % 망간; 0.03 내지 0.5 중량 % 철; 0.01 내지 0.4 중량 % 몰리브덴; 0.01 내지 0.3 중량 % 지르코늄; 0 내지 0.25 중량 % 티타늄; 0 내지 0.25 중량 % 스트론튬; 0 내지 250 ppm 인; 0 내지 4 중량 % 구리 및 10 % 아연; 나머지는 알루미늄 및…
Die vorliegende Erfindung betrifft eine Druckgusslegierung auf der Basis von Aluminium, Magnesium und Silizium bestehend aus: 5,0 bis 7,0 Gew.-% Magnesium; 1,5 bis 7,0 Gew.-% Silizium; 0,3 bis 0,8 Gew.-% Mangan; 0,03 - 0,5 Gew.-% Eisen; 0,01 bis 0,4 Gew.-% Molybdän; 0,01 bis 0.3…
An aluminium, magnesium and silicon-based die casting alloy having 5.0-7.0 wt. % magnesium, 1.5-7.0 wt. % silicon, 0.3-0.8 wt. % manganese, 0.03-0.5 wt. % iron, 0.01-0.4 wt. % molybdenum, 0.01-0.3 wt. % zirconium, 0-0.25 wt. % titanium, 0-0.25 wt. % strontium, 0-250 ppm…
The invention relates to an aluminium, magnesium and silicon-based die casting alloy consisting of: 5.0 - 7.0 wt.-% magnesium; 1.5 - 7.0 wt.% silicon; 0.3 - 0.8 wt.% manganese; 0.03 - 0.5 wt.% iron; 0.01 - 0.4 wt.% molybdenum; 0.01 - 0.3 wt.%zirconium; 0 - 0.25 wt.% titanium; 0…
Die Erfindung betrifft eine Druckgusslegierung auf Aluminium-Silizium Basis mit einer Zusammensetzung bestehend aus: 8,5 bis 11,5 Gew.-% Silizium; 0,1 bis 0,5 Gew.-% Magnesium; 0,3 bis 0,8 Gew.-% Mangan; 0,02 - 0,5 Gew.-% Eisen; 0,005 - 0,5 Gew.-% Zink; 0,02 bis 0,3 Gew.-%…
열처리 후의 파단 연신율 A > 6% 과 동시에 항복점 Rp 0.2 > 200 MPa, 또는 주조 (cast) 상태에서의 높은 파단 연신율 A > 9% 또는 T6 열처리 후의 파단 연신율 > 10% 과 동시에 항복점 Rp 0.2 > 120 MPa 로 증가된 강도를 갖는 구성부품을 위한, 특히 자동차의 구조적 및 섀시 부품을 위한 알루미늄 합금으로서, 9 내지 11.5 중량% 의 규소, 0.5 내지 0.8 중량% 의 망간, 0.2 내지 1.0 중량% 의 마그네슘, 0.1…
본 발명은 다음을 포함하는 주조 합금에 관한 것이다: 철 0.8 내지 3.0 중량%, 마그네슘 0.01 내지 9.0 중량%, 망간 0 내지 2.5 중량%, 베릴륨 0 내지 500 ppm, 티타늄 0 내지 0.5 중량%, 규소 0 내지 0.8 중량%, 스트론튬 0 내지 0.8 중량%, 인 0 내지 500 ppm, 구리 0 내지 4 중량%, 아연 0 내지 10 중량%, 및 니켈, 몰리브덴, 지르코늄, 바나듐, 하프늄, 칼슘, 갈륨 및 붕소로 이루어지는 그룹으로부터 선택되는 0 내지 0.5 중량%의…
An aluminium, magnesium and silicon-based die casting alloy having 5.0-7.0 wt. % magnesium, 1.5-7.0 wt. % silicon, 0.3-0.8 wt. % manganese, 0.03-0.5 wt. % iron, 0.01-0.4 wt. % molybdenum, 0.01-0.3 wt. % zirconium, 0-0.25 wt. % titanium, 0-0.25 wt. % strontium, 0-250 ppm…
The invention relates to an alloy for casting components on an aluminium-magnesium-copper-manganese basis, with a composition consisting of: 5.0 to 9.5% by weight magnesium; 3.0 to 7.5% by weight copper; 1.5 to 4.7% by weight silicon; 0.1 to 1.0% by weight manganese; max. 2% by…
The present disclosure relates to methods, systems, and computer readable media for assessing and displaying respiratory motion. At least one example embodiment provides a method comprising acquiring surface information of a patient using a camera; determining a patient's…
Die Erfindung betrifft eine Gusslegierung mit: Eisen 0,5 0,8 -3,0 Gew. Magnesium 0,01 bis 9,0 Gew. % Mangan 0-2,5 Gew.% Beryllium 0 - 500 ppm Titan 0 - 0,5 Gew. % Silizium 0 - 0,8 Gew. % Strontium 0 - 0,8 Gew. % Phosphor 0 - 500 ppm Kupfer 0 - 4 Gew. % Zink 0 - 10 Gew. % 0- 0,5…
The casting alloy according to the invention is based on aluminum-iron-nickel and consists of the following elements: