By means of additives which decrease the melt viscosity of a binder, a binder composition can be obtained which can be used to obtain shaped bodies of increased strength. By means of additives which decrease the melt viscosity of a binder, a binder composition can be obtained…
Weiler Peter Dr
The use of a non-polymerizable hydroperoxide as radical initiated polymerization regulator in polymerization of ethylenically unsaturated monomers, and containing alkyl and aryl residues, and optionally saturated carbocyclic and heterocyclic rings that can be substituted is new.…
An aqueous dispersion of a polymer is admixed with odor reducing composition of water-soluble compound(s) (A) and optionally water-soluble reducing agent(s). The treated aqueous polymer dispersion is dried to form polymer powder. Compound (A) is preset metal salt, potassium…
Use of protective colloid-stabilized polymer, comprising a protective colloid (I) and a polymer (II), for coating a substrate material with a double-dot coating is claimed.
Use of protective colloid-stabilized polymer, comprising a protective colloid (I) and a polymer (II), for coating a substrate material with a double-dot coating is claimed.
The use of a non-polymerizable hydroperoxide as radical initiated polymerization regulator in polymerization of ethylenically unsaturated monomers, and containing alkyl and aryl residues, and optionally saturated carbocyclic and heterocyclic rings that can be substituted is new.…
By means of additives which decrease the melt viscosity of a binder, a binder composition can be obtained which can be used to obtain shaped bodies of increased strength. By means of additives which decrease the melt viscosity of a binder, a binder composition can be obtained…
Cold molding of particulate materials using a binder (I) comprises pre-heating (I) and material to be bound to 160-240degreesC, and press molding at most 80 degreesC and 1-120 bar to produce molding. (I) comprises polymer powder or aqueous polymer dispersion. The polymer has a…
Cold molding of particulate materials using a binder (I) comprises pre-heating (I) and material to be bound to 160-240degreesC, and press molding at most 80 degreesC and 1-120 bar to produce molding. (I) comprises polymer powder or aqueous polymer dispersion. The polymer has a…
Use of protective colloid-stabilized polymer, comprising a protective colloid (I) and a polymer (II), for coating a substrate material with a double-dot coating is claimed.
Use of a condensation product made from fatty acid and amino functional compound by alkylation of at least partially quaternised product of the condensation product or its mixture, for increasing the volume of paper or carton, is claimed. Independent claims are included for: (1)…
Cold molding of particulate materials using a binder (I) comprises pre-heating (I) and material to be bound to 160-240degreesC, and press molding at most 80 degreesC and 1-120 bar to produce molding. (I) comprises polymer powder or aqueous polymer dispersion. The polymer has a…
By means of additives which decrease the melt viscosity of a binder, a binder composition can be obtained which can be used to obtain shaped bodies of increased strength. By means of additives which decrease the melt viscosity of a binder, a binder composition can be obtained…
Use of protective colloid-stabilized polymer, comprising a protective colloid (I) and a polymer (II), for coating a substrate material with a double-dot coating is claimed.