CN 101,703,965 A#6783679 Most Cited · 14 citations0.9/yr · PR 3.04ActiveCN · Utility
Bauxite column-type floatation method

The invention provides a bauxite column-type floatation method, and relates to bauxite ore-dressing and desilication, in particular to a low-grade diasporite bauxite ore-dressing and desilication method. The method is characterized in that a floatation process comprises the…

CN 102,642,854 A#19727279 Most Cited · 5 citations0.4/yr · PR 1.85ActiveCN · Utility
Treatment method of red mud in Bayer process production flow of aluminum oxide

The invention discloses a treatment method of red mud in Bayer process production flow of aluminum oxide. Red mud generated in the production of aluminum oxide is washed for twice and the red mud flowing at the bottom of a settling tank is subjected to the following steps of:…

CN 101,117,245 A#30307227 Most Cited · 3 citations0.2/yr · PR 1.23ActiveCN · Utility
Method for using reclaimed water in mineral concentration bayer process production

The invention discloses an operation method of an intermediate water produced by a dressing-Bayer process, relating to the method for producing alumina by dressing a bauxite, in particular to the operation method of intermediate water in alumina production process of by…

CN 100,531,945 C#47974495 Most Cited · 1 citations0.1/yr · PR 0.95ActiveCN · Utility
Bauxite tail piling method
Inventors: Yonghong Wang, Dongfeng Zhao, Wei Liu, Erxing Wang, Jiaoping LiuAssignee: China Aluminium Ind Co LtdFiled 2006-08-08 · Granted 2009-08-26

The bauxite tail piling method features that the bauxite tail pulp in 20-70 wt% concentration is first mixed with base material in 10-70 wt% of dry bauxite tail and agglomeration excitant in 0-15 wt% of dry bauxite tail through stirring to form paste in 30-85 wt% concentration;…